Casper Peeters | E-Magy: Does the anode actually stay 20 microns thick? Coin-cell and ZSW pouch-cell swelling data across 100 cycles.

09:41 - 12:01

Other snippets from this talk

Summary of the clip:

Does the anode actually stay 20 microns thick? Coin-cell and ZSW pouch-cell swelling data across 100 cycles.

Starting from a pristine 20-micrometre anode, the first experiment cycled the material at full capacity, 3,600 milliampere-hours per gram. After only 17 cycles the anode had swollen to 32 microns, with extensive cracking. Parts of the anode became disconnected from each other and from the copper layer, so cohesion was lost and the system was no longer workable.

Running the same material at 1,000 milliamps per gram over 100 cycles told a different story: thickness stayed at the original 20 microns. Cohesion inside the material and between particles held, adhesion to the copper layer held, and there was no swelling. That first 100-cycle coin-cell result was described as a good and promising first step.

More advanced measurements followed with ZSW in Germany, using bilayer pouch cells rather than coin cells, with thickness tracked during cycling. Across 100 cycles, thickness variation was less than 1% of the pouch cell and less than 5% of the anode. Against the roughly 300% swelling typical of silicon anodes, that is presented as acceptable proof the swelling problem is solved.

In this short video, you can learn:
* Full-capacity cycling at 3,600 mAh/g swelled a 20-micron anode to 32 microns within 17 cycles, cracking it and breaking contact with the copper layer.
* At 1,000 milliamps per gram the same anode held its 20-micron thickness through 100 cycles with intact particle cohesion and copper adhesion.
* Bilayer pouch cells made with ZSW showed under 1% cell-level and under 5% anode-level thickness variation over 100 cycles, versus 300% for typical silicon anodes.

📋 **Clip Abstract** Full-capacity cycling of a 20-micron anode at 3,600 mAh/g produced 32-micron swelling, cracking and lost copper adhesion after just 17 cycles, while the same material at 1,000 milliamps per gram held its original thickness over 100 cycles. Bilayer pouch cells built with ZSW showed thickness variation below 1% of the cell and below 5% of the anode across 100 cycles, against the 300% typical of silicon anodes.

About the speaker:
* Speaker: Casper Peeters
* Company: E-Magy
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online

Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/

#NanoPorousSilicon, #SiliconDominantAnode, #AnodeSwelling, #PouchCellCycling, #BatteryMaterials, #SolidStateBatteries

This is a highlight of the presentation:

Nano-porous silicon for high-energy silicon-dominant batteries

Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap

Battery Materials: Next-Gen & Beyond Lithium Ion

9-10 February 2022

Online

Organised By:

TechBlick

TechBlick

More Highlights from the same talk.

05:15 - 06:53

Silicon swells on lithiation — how do internal pores plus a crystalline backbone stop the particle expanding outward?

Silicon swells on lithiation — how do internal pores plus a crystalline backbone stop the particle expanding outward?

The particle is built with a nanoporous structure, and two mechanisms together cope with the swelling that would otherwise take place. First, the pores themselves provide the room for expansion. Expansion does occur, but it happens inside the pores — the light green region in the visual representation — so the tendency of the particle to expand outward is reduced.

In parallel, because that internal expansion is accommodated within the particle, part of the silicon remains crystalline. The approach promotes limited-capacity cycling: by limiting capacity to, let's say, 2,000, not all of the silicon lithiates. The fraction that does not react stays crystalline and forms a stable backbone, and with that there is also no expansion.

Together, these are the two mechanisms that limit expansion: pore volume absorbs the volume change internally while the crystalline remnant holds the particle together. The presenter then flags performance as the most important topic for this audience, and says the presentation will go into it in more detail beyond this structural explanation of the particle.

In this short video, you can learn:
* Pores in the nanoporous particle give the silicon room to expand internally instead of pushing the particle outward.
* Limiting cycling capacity to around 2,000 leaves part of the silicon unlithiated and crystalline, forming a stable backbone that does not expand.
* Pore volume and the crystalline backbone are presented as two complementary mechanisms that jointly limit particle expansion.

📋 **Clip Abstract** A nanoporous silicon particle answers swelling with two mechanisms working at once: pores that host the expansion internally, and a crystalline backbone left behind by limited-capacity cycling. Restricting capacity to roughly 2,000 keeps part of the silicon from lithiating, so a stable, non-expanding framework remains inside the particle.

About the speaker:
* Speaker: Casper Peeters
* Company: E-Magy
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online

Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/

#NanoporousSilicon, #CrystallineBackbone, #LimitedCapacityCycling, #PoreVolumeExpansion, #LithiumIonBatteries, #SiliconAnode

15:23 - 17:38

Can structured silicon reach graphite's cost per kilowatt-hour without silane gas or metal-assisted etching?

Can structured silicon reach graphite's cost per kilowatt-hour without silane gas or metal-assisted etching?

The cost target is explicit: introduce the material at a cost comparable to graphite on a kilowatt-hour basis. The rationale is scale—millions of electric vehicles imply hundreds of gigawatt-hours of silicon without increasing price. The precursor is upgraded metallurgical-grade silicon, not necessarily the highest grade; it is abundantly available, reasonably priced and a good starting material for the process.

Manufacturing is kept efficient with few process steps. Silicon is melted, cast onto substrates, and the wafers are further processed. The description emphasizes one machine, not many process steps, followed by a milling step that is more or less industry standard. This equipment leverage matters because it uses known equipment owned in the industry.

The route avoids silane gas, described as expensive and more difficult to transport, which is used in some other processes. It also avoids demanding, complex material engineering with different materials and structures. And it does not use metal-assisted etching to create structured silicon, which suffers from low speed and high cost. These choices address why reaching the required cost structure is difficult.

In this short video, you can learn:
* The target is a silicon-dominant material priced comparably to graphite per kilowatt-hour, with hundreds of gigawatt-hours needed without raising price.
* The process melts upgraded metallurgical-grade silicon, casts it on substrates, processes wafers and uses a standard milling step in one machine.
* It deliberately avoids silane gas, complex multi-material engineering and low-speed, high-cost metal-assisted etching.

📋 **Clip Abstract** The talk sets a graphite-comparable cost per kilowatt-hour for structured silicon at hundreds of gigawatt-hours scale. It uses upgraded metallurgical-grade silicon, a short melt-cast-wafer-mill sequence and avoids silane gas, complex material engineering and metal-assisted etching.

About the speaker:
* Speaker: Casper Peeters
* Company: E-Magy
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online

Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/

#UpgradedMetallurgicalSilicon, #MetalAssistedEtching, #SilaneGasAvoidance, #GraphiteCostParity, #SiliconDominantBatteries, #SolidStateBatteries

08:15 - 09:28

Full silicon anode instead of graphite: how much thinner do the layers get, and what does the stack gain?

Full silicon anode instead of graphite: how much thinner do the layers get, and what does the stack gain?

The starting point is a graphite anode, or graphite with a small amount of silicon oxide, at roughly 350 milliampere-hour per gram. Adding silicon lifts that to as much as 500. In a silicon-dominant system the anode and the layers are much thinner, and across the whole stack — cathode and anode together — the energy density gain reaches 40%.

Thinner layers are not only a packaging effect: the smaller or thinner silicon layers also increase the charge rate of the battery. So the same move that raises anode capacity and shrinks the stack height feeds directly into how fast the cell can be charged, which matters as much as the energy number itself.

A 40% stack-level gain is a design variable, not just a specification. An electric vehicle can carry fewer batteries, giving a compact car that is lower cost and lower weight while driving the same distance — or the same package can be filled with more energy for higher-end sedans and a longer driving range.

In this short video, you can learn:
* Graphite anodes, or graphite with a little silicon oxide, reach about 350 milliampere-hour per gram, while adding silicon pushes anode capacity toward 500.
* Silicon-dominant anodes use much thinner layers and deliver a 40% energy density increase at the level of the full stack.
* Thinner silicon layers also raise the charge rate of the battery, so energy density and charging improve together.

📋 **Clip Abstract** Full-silicon, silicon-dominant anodes replace graphite with much thinner layers, lifting anode capacity from roughly 350 to as much as 500 milliampere-hour per gram and adding 40% energy density to the complete stack. Because the thinner layers also increase charge rate, the gain can be spent either on fewer, cheaper, lighter batteries for compact cars or on more energy and longer driving range for higher-end sedans.

About the speaker:
* Speaker: Casper Peeters
* Company: E-Magy
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online

Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/

#SiliconDominantAnode, #StackLevelEnergyDensity, #AnodeSpecificCapacity, #ThinnerElectrodeLayers, #SiliconAnodeBatteries, #CellStackDesign


About this talk

→ Nano-porous silicon for high-energy silicon-dominant batteries · Casper Peeters · Battery Materials: Next-Gen & Beyond Lithium Ion 2022

More Snippets
CONTACT US

KGH Concepts GmbH

Mergenthalerallee 73-75, 65760, Eschborn

+49 17661704139

admin@techblick.com

TechBlick is owned and operated by KGH Concepts GmbH

Registration number HRB 121362

VAT number: DE 337022439

  • LinkedIn
  • YouTube

Sign up for our newsletter to receive updates on our latest speakers and events AND to receive analyst-written summaries of the key talks and happenings in our events.

Thanks for submitting!

© 2026 by KGH Concepts GmbH

bottom of page