Daisuke Iida | KAUST: Why does InGaN beat phosphide for red micro-LEDs as chip size shrinks?
00:49 - 02:32
Other snippets from this talk
Summary of the clip:
Why does InGaN beat phosphide for red micro-LEDs as chip size shrinks?
Shrinking the micro-LED chip is not neutral for efficiency: external quantum efficiency falls as the chip gets smaller, and the explanation offered here sits on the side of damage. Fabrication itself introduces sidewall damage, and that damage becomes proportionally more important as the emitting area shrinks. The device problem is stated plainly: smaller chip size always means lower efficiency, and this is described as a big problem.
The comparison then turns to materials for red emission, pitting nitride against phosphide. Surface recombination velocity is used as the differentiator between the two material systems: the high-bandgap nitride material shows a much smaller surface recombination velocity, while the phosphide material shows a larger one. That difference in surface behaviour is presented as the basis for comparing how the two material systems behave as chip size changes.
Because of that, the phosphide device degrades sharply when the chip size decreases: its behaviour drops drastically. The nitride material is less severe, showing a more mild external quantum efficiency drop as dimensions come down. That contrast is given as the direct motivation for choosing nitride materials for red micro-LEDs, with the material choice following from the sidewall-limited size dependence rather than from emission wavelength alone.
In this short video, you can learn:
* Smaller micro-LED chips always show lower external quantum efficiency, a problem attributed to damage introduced during device fabrication.
* The high-bandgap nitride material has a much smaller surface recombination velocity than phosphide, which shows a larger one.
* Phosphide EQE drops drastically as chip size shrinks, whereas the nitride drop is milder, which is the stated motivation for nitride red micro-LEDs.
📋 **Clip Abstract** Smaller micro-LED chips lose external quantum efficiency, and the cause is placed on fabrication-induced sidewall damage. Comparing nitride and phosphide for red emission, the nitride system's much smaller surface recombination velocity yields a mild EQE drop against the drastic phosphide roll-off, motivating the choice of InGaN.
About the speaker:
* Speaker: Daisuke Iida
* Company: KAUST
* Event: MicroLED Connect 2024
* Location: High Tech Campus, Eindhoven, Netherlands
Join the most event MicroLED, AR/VR display and Optical I/O Connect event of the year
Learn more https://www.microledconnect.com/
#InGaNMicroLED, #SurfaceRecombinationVelocity, #PhosphideMaterials, #SidewallDamage, #MicroLEDDisplays, #IIIVSemiconductors
This is a highlight of the presentation:
Challenges in InGaN-Based Red Micro-LEDs Technology
More Highlights from the same talk.
05:18 - 07:34
Can AlN barriers strain-compensate InGaN red quantum wells enough to cut dislocation density?
Can AlN barriers strain-compensate InGaN red quantum wells enough to cut dislocation density?
InGaN quantum wells grown on nitride experience huge compressive strain, which makes strain relaxation easy. The proposed strain-compensation concept inserts the opposite strain behavior: aluminum nitride or aluminum-containing nitride in the barrier layer is used to compensate the total strain inside the crystal. In the described profile, inserting the layer lowers the stress, and changing the barrier composition from nitride to aluminum nitride is expected to reduce the total stress.
With lower aluminum content, many defects remain on the surface. As aluminum content in the barrier increases, the surface defects decrease, and lower surface dislocation density is reported when using the aluminum nitride or aluminum-containing barrier structure. This trend links barrier composition directly to defect reduction in the strained InGaN quantum-well structure.
Summarizing, the compensating structure looks good: surface dislocations become lower and lower. The PL intensity becomes stronger and narrower, and the interface is confirmed by X-ray measurement, where the fringes are very sharp when high aluminum content is used in the barrier structure. These results support the strain-compensation approach for InGaN quantum wells.
In this short video, you can learn:
* InGaN quantum wells on nitride suffer huge compressive strain, so inserting opposite-strain AlN or aluminum-containing nitride barriers is proposed to compensate total strain.
* Increasing aluminum content in the barrier reduces surface defects and surface dislocation density compared with lower-aluminum structures.
* The compensated structure shows stronger and narrower PL intensity plus sharp X-ray fringes, confirming improved interface quality at high aluminum content.
📋 **Clip Abstract** Strain compensation for InGaN quantum wells uses aluminum nitride or aluminum-containing nitride barriers to insert opposite strain and reduce total stress in the crystal. Higher aluminum content lowers surface defects and dislocation density, while PL becomes stronger and narrower and X-ray fringes remain sharp, indicating improved interface quality.
About the speaker:
* Speaker: Daisuke Iida
* Company: KAUST
* Event: MicroLED Connect 2024
* Location: High Tech Campus, Eindhoven, Netherlands
Join the most event MicroLED, AR/VR display and Optical I/O Connect event of the year
Learn more https://www.microledconnect.com/
#AlNBarriers, #StrainCompensation, #InGaNRedQW, #SharpXRDFringes, #MicroLEDDisplays, #NitrideSemiconductors
11:00 - 12:52
What single-structure redesign lifted red InGaN EQE to 4.3% and then 1.5× at low current?
What single-structure redesign lifted red InGaN EQE to 4.3% and then 1.5× at low current?
The 2022 result came after modifying the device structure: previously a double-count design, now only one single-count structure. The EQE-versus-current behavior shows a blue line marking 4.3% near the stated current point. This was not a micro-sized device; the standard chip was around 280 by 600 or 800 microns, yet it reached a high optical output-power density.
The emission intensity was comparable to another institute's result, but this is 2022 data. The blue line is almost the same as that 2022 result. In this year, the device was much better at low current density, showing a large EQE position and 1.5 times more enhancement.
At low current, more local emission was obtained, and 645-nanometer emission was reached. The membrane behavior was totally the same, according to the talk. The comparison is between the 2022 blue line and this year’s better low-current-density result; the clip does not give further current or voltage numbers.
In this short video, you can learn:
* A modified structure changed from a double-count design to one single-count structure in the 2022 result.
* The reported EQE reached 4.3% on a standard 280-by-600/800-micron chip, not a micro-sized device.
* This year’s low-current-density result showed a 1.5× EQE enhancement and 645-nanometer emission.
📋 **Clip Abstract** The talk describes a 2022 InGaN red device with a modified structure, moving from double-count to one single-count structure and reaching 4.3% EQE on a standard 280-by-600/800-micron chip. It then reports this year’s better low-current-density behavior, a 1.5× EQE enhancement, unchanged membrane behavior and 645-nanometer emission.
About the speaker:
* Speaker: Daisuke Iida
* Company: KAUST
* Event: MicroLED Connect 2024
* Location: High Tech Campus, Eindhoven, Netherlands
Join the most event MicroLED, AR/VR display and Optical I/O Connect event of the year
Learn more https://www.microledconnect.com/
#InGaNRedMicroLED, #SingleCountStructure, #LowCurrentDensityEQE, #645nmEmission, #MicroLEDDisplays, #InGaNPhotonics
About this talk
→ Challenges in InGaN-Based Red Micro-LEDs Technology · Daisuke Iida · MicroLED Connect 2024