Summary of the clip:
Why are silicon thin films the pouch-cell workhorse, with 88% ICE and 200 cycles at 30 °C?
Amorphous columnar silicon has been studied for years and also works in liquid electrolytes, making it a promising anode. PVD and CVD deposit 100% silicon directly onto the current collector, reaching areal capacities above 3 mA/cm². On lithiation the film grows mainly one-dimensionally in thickness rather than expanding in every direction — attractive for all-solid-state cells, where every interface has to be managed.
Paired with an NMC cathode the thin film is a real workhorse: it allows pouch cells that are easier to handle than lithium metal, with high loadings and room-temperature operation. The initial Coulombic efficiency is 88% and it increases over cycling. Cycling stability is promising, though not yet the 100,000-cycle benchmark cell of Samsung SRJ.
The pouch XS format was the first cell demonstrator, transferring results gained in torque cells — a learning curve, since all layers must be pressurised in a bespoke way. The demonstrator showed 200 cycles, and cycling at 30 °C is also possible, quite nice for a thin-film anode concept.
In this short video, you can learn:
* Columnar silicon takes up lithium by one-dimensional thickness growth instead of expanding in all directions, which simplifies interface management.
* PVD/CVD silicon deposited directly on the current collector gives over 3 mA/cm² areal capacity with 88% initial Coulombic efficiency that rises during cycling.
* Transferring the process from torque cells to a pressurised pouch XS demonstrator achieved 200 cycles, including operation at 30 °C.
📋 **Clip Abstract** Silicon thin films deposited by PVD and CVD give a 100% silicon anode with over 3 mA/cm² areal capacity that lithiates by one-dimensional thickness growth. With an NMC cathode in the pouch XS format the cells reach 88% initial Coulombic efficiency, 200 cycles and 30 °C operation.
About the speaker:
* Speaker: Holger Althues
* Company: Fraunhofer IWS
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online
Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/
#SiliconThinFilmAnode, #ColumnarSilicon, #PVCDeposition, #CoulombicEfficiency, #SolidStateBatteries, #LithiumMetalAnodes
This is a highlight of the presentation:
New anode concepts for solid state batteries
More Highlights from the same talk.
00:50 - 02:14
Why does replacing a liquid electrolyte with a sulfide solid electrolyte alone not raise SSB energy density?
Why does replacing a liquid electrolyte with a sulfide solid electrolyte alone not raise SSB energy density?
The discussion defines solid-state batteries here as sulfidic-based solid electrolytes, not polymer electrolytes. In the scheme, an NMC cathode is laminated on a current collector with conductive additive, and the anode side also has a current collector. The phosphates discussed as promising candidates are ductile and show rather high ionic conductivity. A thin-film, high-volumetric-capacity anode is needed as the active anode material.
If a lithium-ion battery with a graphite anode simply swaps its liquid electrolyte for a solid electrolyte, the result does not gain watt-hours per litre and actually loses watt-hours per kg. That is why the anode active material matters: a thin-film, high-volumetric-capacity anode is required, otherwise the swap alone does not deliver the expected benefit. The clip ties this directly to anode-side and cathode-side design.
Interface engineering between the NMC material and the solid electrolyte is very important, and the separator layer is also a crucial point. Interface engineering on the anode side is emphasized too. These interfaces sit alongside the need for a thin-film, high-volumetric-capacity anode and a sulfidic solid electrolyte, so the cell cannot be treated as a simple liquid-electrolyte swap.
In this short video, you can learn:
* Sulfidic-based solid electrolytes are the definition used here, not polymer electrolytes.
* Simply swapping a graphite-anode lithium-ion cell’s liquid electrolyte for a solid electrolyte does not increase watt-hours per litre and decreases watt-hours per kg.
* A thin-film, high-volumetric-capacity anode plus interface engineering at the NMC/solid-electrolyte and anode sides are presented as necessary.
📋 **Clip Abstract** The clip defines sulfidic-based solid-state batteries and outlines an NMC cathode with conductive additive, current collectors, and a thin-film high-volumetric-capacity anode. It explains that a simple liquid-to-solid electrolyte swap with a graphite anode yields no watt-hours-per-litre gain and a watt-hours-per-kilogram loss, while highlighting NMC/solid-electrolyte, separator, and anode interface engineering.
About the speaker:
* Speaker: Holger Althues
* Company: Fraunhofer IWS
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online
Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/
#SulfidicSolidElectrolyte, #NMCCathode, #ThinFilmAnode, #InterfaceEngineering, #SolidStateBatteries, #LithiumIonBatteries
08:06 - 10:06
How is lithium melt-deposited as a 2–30 µm anode, and why does it short above 0.5 mA/cm²?
How is lithium melt-deposited as a 2–30 µm anode, and why does it short above 0.5 mA/cm²?
A lithophilic layer is generated first on a specially treated copper current collector — nickel also works. Without it, molten lithium forms a droplet and rolls off; there is no wetting, no spreading. With the layer in place, Kai Schöne's melt-deposition method tailors lithium film thickness precisely between 2 and 30 micrometres, and stripping experiments show the deposited amount can be stripped again with a nice correlation.
Implemented into solid-state cells, the films worked — first things first — but stable cycling occurs only at low areal loadings and currents. An intrinsic property of lithium, per the equation cited in the talk, makes dendrite formation more likely at high currents. That is what the team struggles with in these melt-deposited lithium anodes.
Short circuits therefore occur at room temperature, and especially at currents higher than 0.5 milliamps per square centimetre. That ceiling pushed the group to ask what alternatives exist — and to question what happens if a different anode concept is employed instead of melt-deposited lithium thin films on a lithophilic current collector.
In this short video, you can learn:
* A lithophilic layer on copper or nickel is essential, because molten lithium otherwise beads up and rolls off instead of wetting the collector.
* Melt deposition tunes lithium film thickness precisely between 2 and 30 micrometres, and the deposited lithium can be stripped again with a good correlation.
* Stable cycling only holds at low areal loadings and currents; short circuits appear at room temperature above 0.5 milliamps per square centimetre.
📋 **Clip Abstract** Melt deposition of lithium onto a lithophilic-treated copper or nickel current collector gives anodes tuneable from 2 to 30 micrometres, with stripping matching what was deposited. In solid-state cells, however, stable cycling is confined to low areal loadings and currents, with short circuits at room temperature above 0.5 milliamps per square centimetre.
About the speaker:
* Speaker: Holger Althues
* Company: Fraunhofer IWS
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online
Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/
#LithiumMeltDeposition, #LithophilicLayer, #LithiumThinFilm, #DendriteShortCircuit, #SolidStateBatteries, #BatteryMaterials
02:29 - 04:45
What lithium-metal failure modes plague solid electrolytes, and how did a carbon-silver scaffold reach 900 Wh/L?
What lithium-metal failure modes plague solid electrolytes, and how did a carbon-silver scaffold reach 900 Wh/L?
With lithium metal as the anode, the solid electrolyte interface becomes the limiting problem: cycling rate and electrochemical reversibility are restricted. Voids form because a rigid solid electrolyte cannot diffuse into cavities and no liquid can refill them. Lithium also strips and plates as dendrites or mossy lithium, and dendrites can grow along grain boundaries of solid electrolyte particles. Decomposition adds a solid electrolyte interface, especially with phosphate chemistries.
The prominent solution came from Samsung SRJ: a carbon plate matrix with silver nanoparticle sprinkles. This layer and scaffold enable better plating and stripping of lithium. The pouch cell showed 900 Wh/L and 1,000 cycles. But it can only be cycled at elevated temperatures and needs high stack pressure, which is detrimental when OEMs want to implement such batteries in cars.
The concept is a zero-excess anode: lithium solely comes from the NMC and is plated. That framing explains why the scaffold matters—it supports plating and stripping while the cell carries no excess lithium. The remaining constraints are practical: elevated-temperature cycling and continuous stack pressure. For automotive integration, those requirements must be managed, because OEMs need batteries that work without always applying stack pressure.
In this short video, you can learn:
* Voids, dendrites/mossy lithium, grain-boundary dendrite growth and decomposition limit lithium-metal anodes against rigid solid electrolytes.
* Samsung SRJ's carbon plate matrix with silver nanoparticle sprinkles enabled a pouch cell at 900 Wh/L and 1,000 cycles.
* That zero-excess concept still requires elevated temperature and high stack pressure, complicating automotive implementation.
📋 **Clip Abstract** Lithium-metal solid-state anodes suffer voids, dendrite and mossy plating, grain-boundary penetration and decomposition, limiting rate and reversibility. Samsung SRJ addressed plating and stripping with a carbon plate matrix plus silver nanoparticle sprinkles, reaching 900 Wh/L and 1,000 cycles in a pouch cell, but only with elevated temperature and high stack pressure.
About the speaker:
* Speaker: Holger Althues
* Company: Fraunhofer IWS
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online
Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/
#ZeroExcessAnode, #CarbonPlateMatrix, #SilverNanoparticleSprinkles, #900WhPerL, #SolidStateBatteries, #LithiumMetalAnodes
About this talk
→ New anode concepts for solid state batteries · Holger Althues · Battery Materials: Next-Gen & Beyond Lithium Ion 2022
Other talks by Holger Althues
- Evaluation of columnar Silicon anodes in high energy Lithium-Ion- and solid state battery cells · Solid-State Batteries: Innovations, Promising Start-Ups, & Future Roadmap 2024