Muhammad Fatahilah | Coherent Corp.: How do you release microLEDs from sapphire selectively, with sub-1.5 µm placement, at 500,000 dice per 40 seconds?
02:14 - 04:17
Other snippets from this talk
Summary of the clip:
How do you release microLEDs from sapphire selectively, with sub-1.5 µm placement, at 500,000 dice per 40 seconds?
The process uses a 248 nm excimer laser with five electron volts, absorbed by gallium nitride but not sapphire. A lift transfers the epi wafer to chip-on-carrier one, contact facing down, coated with residue-free adhesive no thicker than 300 nanometers. Wafer bonding then debonding follows, while chip-on-carrier two receives no laser process before transfer to a final carrier such as PCB.
The final transfer uses low energy density lift around 100 millijoules per square centimeter. A dedicated machine transfers at least half a million dice in 40 seconds. With three sigma, pitch error stays below 1.5 micrometer, and the process can reach eight-inch wafers. Demonstrated here are four-inch and six-inch wafers, with 20 by 10 micrometer microLEDs from the chip-on-carrier one wafer.
High precision and high throughput emerge from this residue-free laser lift process. The next generation two system can go to one million, extending the demonstrated half-million dice per 40 seconds. Selective gallium nitride removal from sapphire avoids processing the sapphire directly, while the thin residue-free adhesive enables bonding, debonding and carrier transfer.
In this short video, you can learn:
* A 248 nm excimer laser's five electron volts are absorbed by gallium nitride but not sapphire, enabling selective removal.
* Residue-free adhesive with a maximum 300 nanometer thickness supports wafer bonding and debonding before chip-on-carrier two transfer.
* The dedicated machine transfers at least 500,000 dice in 40 seconds with three-sigma pitch error below 1.5 micrometer, scaling to eight-inch wafers and one million next generation.
📋 **Clip Abstract** The process selectively removes gallium nitride from sapphire using a 248 nm excimer laser, because the five electron volts are absorbed by gallium nitride but not sapphire. A residue-free adhesive under 300 nanometers, low energy density lift around 100 millijoules per square centimeter, and a machine achieve at least half a million dice per 40 seconds with three-sigma pitch error below 1.5 micrometer.
About the speaker:
* Speaker: Muhammad Fatahilah
* Company: Coherent Corp.
* Event: nnovation Festival: Additive, Printed, Sustainable Electronics, MicroLEDs and AR/VR Displays, Perovskites | July 2026
* Location: Online Platform
Annual access to our onsite event(s), all online events and a library featuring over 1800 presentations (recordings + PDF) across all our onsite and onsite events and technology areas. Join us and over 2000 members from around the world now.
Explore and join now --> https://www.techblick.com/
#ExcimerLaser248Nm, #ResidueFreeAdhesive, #GalliumNitrideRemoval, #Below1Point5MicronPitch, #MicroLEDManufacturing, #HeterogeneousIntegration
This is a highlight of the presentation:
Residue-Free Laser-Induced Forward Transfer of MicroLEDs
More Highlights from the same talk.
05:35 - 07:38
A 300 nm process left 60 nm residue — so how thin must the process go for a clean microLED lift?
A 300 nm process left 60 nm residue — so how thin must the process go for a clean microLED lift?
The process removes dice at 448 nanometer with low energy density, then transfers COC2 to a standard receiver. A 2x2 transfer uses step and repeat, while fly and apply can place half a million in 45 seconds. The 45 by 40 micrometer dice land on the final substrate clearly, so the next question is residue.
To check residue, a second exposure is done on dice that landed on the final substrate. At 300 nanometer frequency, residue remains, not visible to the naked eye after processing. The LSM measurement done on site shows around 60 nanometer residue. The question becomes why not make it smaller or thinner.
They decide to go thinner, to 40 nanometer, and fortunately no residue is seen again. That means the lift process transfers from SiLC-II and can produce a clean die after lift, so no post-cleaning is needed. This is really promising for the mass transfer process.
In this short video, you can learn:
* At 300 nanometer frequency, LSM showed around 60 nanometer residue.
* Reducing the layer to 40 nanometer eliminated residue and removed the need for post-cleaning after lift.
* The lift process transfers 45 by 40 micrometer dice from SiLC-II to the final substrate, with fly and apply reaching half a million in 45 seconds.
📋 **Clip Abstract** At 448 nanometer and low energy density, dice are removed and COC2 is transferred to a standard receiver, with 2x2 step-and-repeat and fly-and-apply placing half a million in 45 seconds. After transfer, 300 nanometer processing leaves around 60 nanometer residue by LSM, but thinning to 40 nanometer gives clean dice after lift and no post-cleaning.
About the speaker:
* Speaker: Muhammad Fatahilah
* Company: Coherent Corp.
* Event: nnovation Festival: Additive, Printed, Sustainable Electronics, MicroLEDs and AR/VR Displays, Perovskites | July 2026
* Location: Online Platform
Annual access to our onsite event(s), all online events and a library featuring over 1800 presentations (recordings + PDF) across all our onsite and onsite events and technology areas. Join us and over 2000 members from around the world now.
Explore and join now --> https://www.techblick.com/
#SiLCII, #COC2, #StepAndRepeat, #ResidueFreeLift, #MicroLEDDisplays, #SemiconductorManufacturing