Nicolo Brambilla | Nanoramic Laboratories: How does a 3D carbon matrix replace PVDF and raise cathode conductivity 10–100×?
02:10 - 03:14
Other snippets from this talk
Summary of the clip:
How does a 3D carbon matrix replace PVDF and raise cathode conductivity 10–100×?
The active layer is the coating applied to both anode and cathode on top of aluminum or copper foil. Within that layer, a 3D carbon matrix serves as the electrical scaffold. In cathodes, measured electrical conductivities are between 10 and 100 times higher than a conventional composite of PVDF binder plus carbon black.
The same 3D carbon matrix also has binding properties. This dual function matters because the structure provides high electrical conductivity that is uniform throughout the active layer while still binding the layer. That combination is why and how the cathode can completely eliminate the need for PVDF binders.
Uniform conductivity throughout the active layer is a key aspect. The matrix is not only an electrical scaffold; it also supplies binding. With both high conductivity and binding in the coating, the cathode no longer requires a separate PVDF binder. The measured 10–100× conductivity advantage is against a PVDF-plus-carbon-black composite.
In this short video, you can learn:
* The active layer is coated on both anode and cathode over aluminum or copper foil.
* A 3D carbon matrix acts as an electrical scaffold and provides binding properties in the coating.
* Cathode conductivity is measured 10–100× higher than a PVDF binder plus carbon black composite, enabling PVDF elimination.
📋 **Clip Abstract** A 3D carbon matrix in the active layer provides both electrical scaffolding and binding. In cathodes it delivers 10–100× higher conductivity than a PVDF binder plus carbon black composite, uniform throughout the layer, allowing complete elimination of PVDF binders.
About the speaker:
* Speaker: Nicolo Brambilla
* Company: Nanoramic Laboratories
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online
Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/
#3DCarbonMatrix, #PVDFFreeCathode, #ActiveLayerConductivity, #CarbonBlackComposite, #LithiumIonBatteries, #BatteryElectrodes
This is a highlight of the presentation:
Silicon-Dominant and NMC Electrodes Through an NMP-free/ PVDF-free Process for High Energy Li-ion Batteries
More Highlights from the same talk.
06:58 - 08:18
Why can NMP-free slurries dry 40% faster at 65°C and simplify solvent recovery?
Why can NMP-free slurries dry 40% faster at 65°C and simplify solvent recovery?
Two slurry chemistries are used: water-based and alcohol-based. Both are formulated to dry more readily than NMP-based cathode slurries, which changes how existing equipment is run. On a roll-to-roll coater already in place, the cathode can be processed at about 65°C instead of 150°C, cutting the thermal burden on the line without changing the tooling concept.
For greenfield factories the drying advantage becomes a sizing argument: matching the throughput of a previous line requires a smaller coating system, because the slurry releases its solvent more easily. Measured on a given machine at equal loadings, the NMP-free coating dries 40% faster — significant given that the cathode is the most expensive part of the cell, in material and in process cost.
Solvent handling is where the chemistry diverges. Recovery hardware is itself expensive, and a water-based process removes the need for it entirely, while alcohol-based slurries need a much simpler recovery system than NMP requires. That flexibility matters as much as the drying rate, because it shifts capital and operating cost out of the coating step rather than merely speeding it up.
In this short video, you can learn:
* NMP-free slurries let an existing roll-to-roll coater run the cathode at roughly 65°C instead of 150°C.
* At equal loadings on the same machine the NMP-free coating dries 40% faster, and a new line needs a smaller coater to match prior throughput.
* Water-based slurries eliminate the solvent recovery system entirely, while alcohol-based slurries need a much simpler one than NMP.
📋 **Clip Abstract** Water-based and alcohol-based cathode slurries dry at about 65°C instead of 150°C on existing roll-to-roll coaters, and dry 40% faster at equal loadings. Solvent recovery is simplified — eliminated for water, much reduced for alcohol — in a process where the cathode carries both the highest material and process cost.
About the speaker:
* Speaker: Nicolo Brambilla
* Company: Nanoramic Laboratories
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online
Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/
#NMPFreeSlurry, #AlcoholBasedSlurry, #CathodeDrying, #SolventRecovery, #LithiumIonBatteries, #BatteryCellManufacturing
14:54 - 16:42
What do 9 Ah silicon-dominant cells deliver in energy density, swelling and 1,000-cycle retention?
What do 9 Ah silicon-dominant cells deliver in energy density, swelling and 1,000-cycle retention?
The multilayer 9 Ah cells, described as small-to-medium format, deliver more than 315 Wh/kg and more than 820 Wh/L even with a non-optimized package. The speaker notes these values are measured not only internally but also by third parties. The cells are presented as a demonstration rather than a packaging-optimized product, so the reported gravimetric and volumetric figures are tied to that non-optimized package.
From 0% to 100% state of charge, the cell expands about 8%. Cycle life is described as pretty stable considering the amount of silicon, reaching about 70% after 1,000 cycles at room temperature. These swelling and retention data frame the practical trade-off for silicon loading in 9 Ah multilayer cells, while the package remains unoptimized.
Fast charging reaches more than 80% state of charge, referenced to actual capacity measured at C/3, in less than 15 minutes. The test runs from 5% to 100% SOC using CCCB charging at 25°C, not elevated temperature, and the speaker highlights the cell loadings. More recent data in larger cells is mentioned but not quantified in this clip.
In this short video, you can learn:
* The 9 Ah multilayer cells exceed 315 Wh/kg and 820 Wh/L with a non-optimized package, including third-party measurements.
* The cells expand about 8% from 0% to 100% SOC and retain about 70% after 1,000 cycles at room temperature.
* Fast charging reaches over 80% SOC in under 15 minutes from 5% to 100% SOC using CCCB at 25°C.
📋 **Clip Abstract** Nine-amp-hour multilayer cells are reported at more than 315 Wh/kg and 820 Wh/L in a non-optimized package, with third-party measurements. They show about 8% expansion from 0% to 100% SOC, roughly 70% retention after 1,000 room-temperature cycles, and over 80% SOC in under 15 minutes via CCCB charging at 25°C.
About the speaker:
* Speaker: Nicolo Brambilla
* Company: Nanoramic Laboratories
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online
Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/
#SiliconDominantAnode, #CCCBCharging, #CellSwelling, #NineAmpHourCells, #LithiumIonBatteries, #BatteryCycleLife
09:40 - 10:46
Can a silicon anode with LFP reach $50/kWh at cell level while fixing LFP's energy-density drawback?
Can a silicon anode with LFP reach $50/kWh at cell level while fixing LFP's energy-density drawback?
The clip reports a silicon-anode/LFP combination reaching $50 per kilowatt-hour at cell level. The claimed enabler is high loading on the cathode side, which the speaker says lets the cell overcome LFP’s main drawback: energy density. That positions the silicon anode specifically for LFP batteries rather than only high-energy NMC designs, while retaining good performance.
On NMC, the same silicon-anode approach is said to deliver 350 watt-hour per kilogram and lower cost, quoted at $70 per kilowatt-hour with the silicon anode. The speaker presents these as an all-in-one cell: high energy, lower cost and fast charging. The stated fast-charge result is 15 minutes to 80%, with data promised later in the presentation.
The comparison is framed at cell level, not pack level: $50/kWh for silicon anode plus LFP and $70/kWh for silicon anode plus NMC. The speaker emphasizes that lower costs are achieved in the same cell and that the LFP route can achieve high cathode loading. These are spoken claims from the presentation, with later data referenced for fast charging.
In this short video, you can learn:
* A silicon-anode/LFP cell is claimed to reach $50/kWh at cell level with high cathode loading.
* The silicon-anode/NMC cell is claimed to deliver 350 Wh/kg and $70/kWh.
* Fast charging is stated as 15 minutes to 80%, with data to be shown later.
📋 **Clip Abstract** The talk segment links silicon-anode cells to two cost/performance targets: $50/kWh with LFP at cell level and $70/kWh with NMC at 350 Wh/kg. It also cites high cathode loading to address LFP energy density and states 15-minute charging to 80%, with data promised later.
About the speaker:
* Speaker: Nicolo Brambilla
* Company: Nanoramic Laboratories
* Event: Solid-State Batteries: Innovations, Promising Start-ups, Future Roadmap
* Location: Online
Join TechBlick to learn about the state of the art in solid state batteries, Si anode, advanced cathodes, sodium batteries, and beyond
https://www.techblick.com/
#SiliconAnodeLFP, #HighLoadingCathode, #350WhKgNMC, #15MinuteFastCharge, #LithiumIonBatteries, #EnergyDensity
About this talk
→ Silicon-Dominant and NMC Electrodes Through an NMP-free/ PVDF-free Process for High Energy Li-ion Batteries · Nicolo Brambilla · Battery Materials: Next-Gen & Beyond Lithium Ion 2022