How do PbS quantum-dot sizes tune SWIR cut-off from 940 to 1550 nm, and can 200 mm wafer processing make them manufacturable?
Lead sulfide quantum dots absorb according to nanocrystal size, so the same silicon platform delivers cut-off wavelengths at 940, 1450 and 1550 nm. Each device needs its transport layers and full stack re-optimised to reach quantum efficiency above 40–50% at the peak absorption. All of these devices also absorb in the visible; depending on the application that visible response can be used or filtered out, but optimisation always targets the peak.
The next step is transferring the process to full wafers, the only route to economy of scale plus the uniformity and throughput advantage. That work is running in a 200 mm fab, with a process that can be ported to 300 mm later. The trick is respecting every semiconductor fab constraint: contamination, design rules and the permitted materials.
On 5-micrometer pixel pitch arrays, every coating layer of the quantum dot stack is deposited and patterning techniques pixelate the stack. The zoom shows a chocolate bar structure: each pixel cleanly separated from its neighbours, the quantum dot layer nicely embedded in the stack. These full image sensors are already built on the real readout on 200 mm wafers — work in progress, but moving.
In this short video, you can learn:
* Sizing lead sulfide nanocrystals shifts the absorption cut-off from 940 to 1450 and 1550 nm on the same silicon platform.
* Each wavelength needs its own transport-layer and stack optimisation to hold quantum efficiency above 40–50%.
* A 200 mm fab process, portable to 300 mm, has produced 5-micrometer pitch pixelated quantum dot stacks on real readout wafers.
📋 **Clip Abstract** Lead sulfide quantum dots on silicon are tuned by nanocrystal size to cut off at 940, 1450 and 1550 nm, with the stack re-optimised per wavelength for quantum efficiency above 40–50%. Moving to a 200 mm fab — and later 300 mm — with 5-micrometer pitch patterning yields pixel-isolated stacks on real readout, though the full image sensors remain work in progress.
About the speaker:
* Speaker: Pawel Malinowski
* Company: IMEC
* Event: Quantum Dots 2021
* Location: Online
Join TechBlick - the home of frontier display technologies such as microLEDs, AR/VR, quantum dots, and beyond
https://www.techblick.com/
#PbSQuantumDots, #SWIRCutoffTuning, #200mmWaferProcessing, #ChocolateBarPixelation, #ShortWaveInfraredImaging, #QuantumDotPhotodetectors
This is a highlight of the presentation:
High Pixel Density Infrared Sensors Enabling Augmented Vision
More Highlights from the same talk.
04:17 - 05:42
Can thin-film SWIR sensors beat $10,000–15,000 III-V/II-VI cameras on cost while matching performance?
Can thin-film SWIR sensors beat $10,000–15,000 III-V/II-VI cameras on cost while matching performance?
Standard CMOS image sensors sit below III-V options: mature, high-throughput and low-cost at roughly 6 billion units per year, with very small pixels and design flexibility. Their silicon limits sensitivity in the shortwave IR. That gap pushes shortwave-IR absorption into III-V or II-VI absorbers integrated above readouts, usually by flip-chip hybridization.
That absorber route is expensive: high-temperature epitaxy grows the absorber layer first, then the wafer is processed, the readouts need special processing, and the two must be connected. The result is a high application bar, low throughput, and cameras costing upwards of $10,000 to $15,000. It is very mature, used for decades, and works great.
TFPD enters as the thin-film option; the clip places this class between standard CIS/CMOS and III-Vs. It is discussed against the same benchmarks: CMOS maturity, 6-billion-unit scale, and small-pixel design flexibility on one side; flip-chip III-V/II-VI hybridization, high-temperature epitaxy, special readout processing, low throughput, and $10,000–$15,000 cameras on the other. The thin-film route is the alternative being assessed.
In this short video, you can learn:
* CMOS image sensors reach about 6 billion units per year with very small pixels and design flexibility, but silicon blocks shortwave-IR sensitivity.
* III-V/II-VI shortwave-IR absorbers require high-temperature epitaxy, special readout processing and flip-chip connection, driving cameras to $10,000–$15,000 with low throughput.
* TFPD uses a thin-film approach and is positioned between standard CIS/CMOS and mature III-V/II-VI detector technology.
📋 **Clip Abstract** The clip contrasts mature CMOS image sensors—roughly 6 billion units per year, very small pixels and low cost from scale—with III-V/II-VI shortwave-IR absorbers that need high-temperature epitaxy, special readout processing and flip-chip hybridization. It frames TFPD as the thin-film option between them, set against $10,000–$15,000 III-V/II-VI cameras, low throughput and a high application bar.
About the speaker:
* Speaker: Pawel Malinowski
* Company: IMEC
* Event: Quantum Dots 2021
* Location: Online
Join TechBlick - the home of frontier display technologies such as microLEDs, AR/VR, quantum dots, and beyond
https://www.techblick.com/
#CMOSImageSensors, #FlipChipHybridization, #HighTemperatureEpitaxy, #SWIRSensitivity, #InfraredImaging, #Photodetectors
22:14 - 23:37
Cu-Cu-bonded InGaAs versus quantum-dot SWIR: competing for the same pixels, or two different sensitivity tiers?
Cu-Cu-bonded InGaAs versus quantum-dot SWIR: competing for the same pixels, or two different sensitivity tiers?
The copper bonding in Sony's sensor draws open admiration — it is called absolutely beautiful. Its indium gallium arsenide absorber is credited with currently the highest quantum efficiency, or one of the highest external quantum efficiencies, among the approaches discussed. That makes it the obvious route wherever an application genuinely needs high sensitivity and high EQE. InGaAs is treated as the performance benchmark, not a technology being written off.
SWIR is described as an emerging field that everybody is talking about, with a lot happening and several competing approaches visible at events such as TechBlick. Quantum dots are positioned as the enabler that brings SWIR functionality into more consumer devices and into many new machine vision applications. With further development, the speaker suggests, automotive could follow. The emphasis is on broadening access rather than chasing the highest possible sensitivity.
For quantum dots the target is explicitly small footprints and quality that is good enough for the application, not record EQE. The conclusion is that there is place for both: quantum dots are not intended to replace indium gallium arsenide, but to play where InGaAs is either not needed or, as the answer breaks off, where it is not the right fit.
In this short video, you can learn:
* Sony's copper-bonded InGaAs sensor is admired as beautiful engineering and credited with currently the highest or near-highest EQE.
* SWIR is an emerging field with many competing approaches, and quantum dots are pitched as the enabler for consumer devices, new machine vision and, later, automotive.
* Quantum dots target small footprints and good-enough quality, and are not meant to replace InGaAs, so both have a place.
📋 **Clip Abstract** A comparison of Sony's copper-bonded InGaAs SWIR sensor with quantum-dot alternatives, framed by external quantum efficiency and application fit. InGaAs keeps the high-sensitivity, high-EQE territory while quantum dots pursue small-footprint consumer and machine vision volume.
About the speaker:
* Speaker: Pawel Malinowski
* Company: IMEC
* Event: Quantum Dots 2021
* Location: Online
Join TechBlick - the home of frontier display technologies such as microLEDs, AR/VR, quantum dots, and beyond
https://www.techblick.com/
#InGaAsEQE, #QuantumDotSWIR, #CuCuBonding, #SmallFootprintSensors, #SWIRImaging, #MachineVision
11:14 - 12:06
How small can SWIR pixels get, and what does scaling from 5 µm to 1.82 µm buy in resolution and die footprint?
How small can SWIR pixels get, and what does scaling from 5 µm to 1.82 µm buy in resolution and die footprint?
The starting point is a 5 µm pixel pitch, described as the smallest reported for indium gallium arsenide hybridization. Moving to 130 nm nodes enabled 2.5 µm pixels. In the line-pair images, the finer pitch makes neighboring lines much easier to recognize, giving much better detail resolution. That links pixel scaling directly to image quality, not just array count.
Further test arrays reached 2.1 µm and 1.82 µm, cited as the smallest arrays for SWIR. The benefit is twofold: improved resolution from smaller pixels, and the ability to squeeze many, many more pixels onto the same wafer by scaling down. The SWIR context also matters because the part does not reflect in SWIR, so real can be distinguished from fake.
The progression from 5 µm to 2.5 µm, then to 2.1 µm and 1.82 µm, shows a scaling path for SWIR sensor arrays. Each step is presented with a concrete pixel pitch and, for the 2.5 µm case, a visible line-pair resolution gain. The 1.82 µm arrays are framed as the smallest for SWIR, while wafer-level packing gains come from scaling down.
In this short video, you can learn:
* A 5 µm pixel pitch is reported as the smallest for indium gallium arsenide hybridization, with 130 nm nodes enabling 2.5 µm pixels.
* Line-pair images show that the 2.5 µm pitch resolves neighboring lines much better than the 5 µm starting point.
* Test arrays at 2.1 µm and 1.82 µm are cited as the smallest for SWIR, and scaling down allows many more pixels on the same wafer.
📋 **Clip Abstract** SWIR pixel scaling moves from a 5 µm pitch, the smallest reported for indium gallium arsenide hybridization, to 2.5 µm using 130 nm nodes. Test arrays at 2.1 µm and 1.82 µm are cited as the smallest for SWIR, with line-pair images showing better detail resolution and wafer-level scaling packing many more pixels.
About the speaker:
* Speaker: Pawel Malinowski
* Company: IMEC
* Event: Quantum Dots 2021
* Location: Online
Join TechBlick - the home of frontier display technologies such as microLEDs, AR/VR, quantum dots, and beyond
https://www.techblick.com/
#InGaAsHybridization, #SWIRPixelPitch, #LinePairResolution, #Sub2MicronSWIR, #InfraredSensors, #SWIRImaging
About this talk
→ High Pixel Density Infrared Sensors Enabling Augmented Vision · Pawel Malinowski · Quantum Dots: Material Innovations, Commercial Applications 2021