top of page
Bringing performance of SAC solder to low temperature substrates
Printed, Hybrid, InMold, and 3D Electronics 2022
8 March 2022
Online
TechBlick Platform
Watch the 5-minute excerpt from the talk
▶ Video highlights from this talk
- ▶ How can SAC305, normally a +240°C alloy, reflow in the low-temperature soldering range?
- ▶ Can supercool liquid metal microcapsules wet an unmelted SAC305 solder ball and underlying copper contact pad at 180°C?
- ▶ Do these assembled BGA solder joints survive 1,000 thermal shocks from -40 to 110°C with no failures?
More video highlights from Ian Tevis
- ▶ How can ordinary solder alloys stay liquid far below their melting point and then form interconnects on demand? · Printed, Hybrid, Structural & 3D Electronics 2021
- ▶ How low can a 62°C indium-tin-bismuth solder be supercooled, and what processing range does that unlock? · Printed, Hybrid, Structural & 3D Electronics 2021
- ▶ Can SAC305 and bismuth-tin reflow at 165°C and 120°C without changing alloy composition? · Printed, Hybrid, Structural & 3D Electronics 2021
Other talks by Ian Tevis
- Supercooled Fully Metallic FHE Interconnect Technology · Printed, Hybrid, Structural, & 3D Electronics 2021
bottom of page