top of page

Ian Tevis

SAFI-Tech

* All members of the platform can watch the entire presentation.

 

Please register to become a member.

Ian Tevis | SAFI-Tech: How can SAC305, normally a +240°C alloy, reflow in the low-temperature soldering range?

00:20 - 01:41

Other snippets from this talk

Summary of the clip:

How can SAC305, normally a +240°C alloy, reflow in the low-temperature soldering range?

The materials are familiar solder metal alloys such as SAC305 and bismuth tin, encapsulated as microcapsules. Each microcapsule has a core-shell structure: the core is the regular solder metal alloy, while a proprietary shell—a nano film on the microcapsule surface—keeps that metal in its molten, melted liquid state. This encapsulation is the starting point for reflowing the alloy without changing its identity.

During reflow, liquid metal can come out of the shell and wet with other little microcapsules. It can also wet substrates and flow out, eventually turning solid to form a solder joint. That joint comes from the exact solder metal alloy, with the same melting point and similar microstructures and properties as the bulk metal alloy.

The approach is described as a platform technology that can extend the processing range of different solder metals. Two targets are SAC305 and bismuth tin. SAC305 is brought down from its normal high +240°C temperature into the LTS, low temperature soldering, range—normally dominated by bismuth tin-based solders. It also points to the other side of that processing range.

In this short video, you can learn:
* SAC305 and bismuth tin are encapsulated as core-shell microcapsules with a proprietary nano-film shell.
* The shell keeps the solder alloy molten until liquid metal wets other microcapsules and substrates, then solidifies into a joint.
* The platform brings SAC305 down from +240°C into the LTS range, while the resulting joint keeps the exact alloy's melting point and similar microstructure and properties.

📋 **Clip Abstract** SAC305 and bismuth tin are encapsulated in core-shell microcapsules whose proprietary nano-film shell holds the alloy in a molten liquid state. On reflow, the liquid metal wets other microcapsules and substrates, solidifies into a joint from the exact alloy, and lets SAC305 be processed down from +240°C into the LTS range.

About the speaker:
* Speaker: Ian Tevis
* Company: SAFI-Tech
* Event: Printed, Hybrid, InMold, and 3D Electronics
* Location: Online

#SAC305, #BismuthTin, #CoreShellMicrocapsules, #LowTemperatureSoldering, #PrintedElectronics, #ElectronicPackaging

This is a highlight of the presentation:

Bringing performance of SAC solder to low temperature substrates

Printed, Hybrid, InMold, and 3D Electronics

​

9-10 March 2022

Online

Organised By:

TechBlick

​

More Highlights from the same talk.

02:14 - 03:26

Can supercool liquid metal microcapsules wet an unmelted SAC305 solder ball and underlying copper contact pad at 180°C?

Can supercool liquid metal microcapsules wet an unmelted SAC305 solder ball and underlying copper contact pad at 180°C?

SAC305 supercool liquid metal microcapsules can be soldered to a SAC305-based ball grid array at 180°C, and processing can even occur as low as 165°C. This soldering temperature is 40°C below the melting point of SAC305. Cross-sections reveal that the supercooled liquid metal material successfully wets a non-collapsed SAC305 solder ball without requiring the solder ball itself to melt during processing.

Because the liquid metal inside the microcapsules is already in a molten state at 180°C, it can wet adjacent metallic structures even when they remain solid. The material wets the non-collapsed SAC305 solder ball, forms a solder joint, and wets the underlying copper contact pad. This enables full joint formation well below standard SAC305 reflow temperatures.

Supercool liquid metal microcapsules composed of SAC alloy demonstrate every critical mechanism required in a solder joint at 180°C, including coalescence, solder ball wetting, and intermetallic compound growth. Assemblies prepared with this technology were sent for external validation, where they underwent thermal shock testing to evaluate the structural integrity and reliable bonding of the low-temperature joints.

In this short video, you can learn:
* SAC305 supercool liquid metal microcapsules form joints with SAC305 ball grid arrays at 180°C, or as low as 165°C.
* The already molten microcapsules wet both a non-collapsed SAC305 solder ball and the underlying copper contact pad 40°C below SAC305's melting point.
* Supercooled liquid metal microcapsules complete coalescence, solder ball wetting, and intermetallic compound formation at 180°C and undergo external validation through thermal shock testing.

📋 **Clip Abstract** Supercool liquid metal microcapsules enable SAC305 soldering onto ball grid arrays at 180°C—40°C below the melting point of standard SAC305—and as low as 165°C. The process achieves complete coalescence, solder ball wetting, copper pad wetting, and intermetallic compound formation while leaving the target SAC305 solder ball non-collapsed.

About the speaker:
* Speaker: Ian Tevis
* Company: SAFI-Tech
* Event: Printed, Hybrid, InMold, and 3D Electronics
* Location: Online

#LiquidMetalMicrocapsules, #LowTemperatureSoldering, #BallGridArray, #IntermetallicCompounds, #HybridElectronics, #PrintedElectronics

02:21 - 03:33

How can ordinary solder alloys stay liquid far below their melting point and then form interconnects on demand?

How can ordinary solder alloys stay liquid far below their melting point and then form interconnects on demand?

Solder metal alloys are formed into particles: a core of regular solder metal alloy covered by a very thin shell, part native oxide of the metal and part organic layer. That microcapsule form factor gives anyone trying to make interconnects the ability to supercool the alloy, keeping it liquid well below the normal melting point.

Squish these little microcapsules mechanically, or dissolve that shell, and the liquid metal flows out to form an interconnect at dramatically lower processing temperatures. Rupture is the trigger, not bulk heating of the deposit. Processing heat drops well below the alloy's rated melting point, and sometimes parts can be joined at ambient temperatures.

Alloy choice stays familiar. SAC305, standard in the rigid electronics space, can be made into this form factor, and so can the bismuth-tin solders some people in the space are examining. Pretty much any solder metal alloy can be turned into microcapsules, used on demand, and processed at lower heat.

In this short video, you can learn:
* Microcapsules hold a standard solder alloy liquid well below its normal melting point by enclosing the core in a thin native-oxide or organic shell.
* Mechanical squishing or dissolution of that shell releases the liquid metal, which forms an interconnect at dramatically lower processing temperatures, sometimes as low as ambient.
* SAC305 and bismuth-tin solders can both be converted into this microcapsule form factor and used on demand.

📋 **Clip Abstract** Solder metal alloys are encapsulated in a very thin native-oxide or organic shell so the core can be supercooled and kept liquid far below the alloy's melting point. Breaking or dissolving that shell releases the metal to form an interconnect at dramatically lower processing temperatures, with SAC305 and bismuth-tin alloys included and ambient joining sometimes possible.

About the speaker:
* Speaker: Ian Tevis
* Company: SAFI-Tech
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online

Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/

#SupercooledSolderMicrocapsules, #SAC305, #BismuthTinSolder, #AmbientInterconnectFormation, #PrintedElectronics, #AdvancedPackaging

03:22 - 04:45

Do these assembled BGA solder joints survive 1,000 thermal shocks from -40 to 110°C with no failures?

Do these assembled BGA solder joints survive 1,000 thermal shocks from -40 to 110°C with no failures?

External validation subjected assembled BGA joints to thermal shock testing from -40°C to 110°C for 1,000 cycles. Every assembled BGA solder joint remained conductive with no failures. The result is attributed to a true metallurgical solder joint: diffusion between the tin-based solder material and the SAC305 ball. The joint forms through intermetallic compound growth, which the talk identifies as the mechanism behind the zero-failure thermal-shock outcome.

The joint relies on intermetallic compound formation between the tin-based solder and SAC305 and the copper-based substrate underneath. The talk names the phase as a classic copper-6, tin-5 intermetallic compound—well known, well understood, and expected to form. Its average thickness is about 2.5 micrometers. That is described as being on the lower end, yet still a reliable solder joint.

Beyond SAC305, the work moves to bismuth-tin, a low-temperature solder that can be brought down to 110°C. At that temperature, the process solders rigid components to silver traces on PET. The final slide shows a filleted solder structure formed between a rigid component and that flexible silver trace on PET, with a classic bismuth-tin microstructure in the solder.

In this short video, you can learn:
* Assembled BGA joints remained conductive with no failures after 1,000 thermal shocks from -40°C to 110°C.
* The joint is a true metallurgical bond formed by diffusion and intermetallic compound growth between tin-based solder and the SAC305 ball.
* Bismuth-tin solder can be brought to 110°C to join rigid components to silver traces on PET, forming a filleted structure with classic bismuth-tin microstructure.

📋 **Clip Abstract** External validation of assembled BGA joints showed no failures after 1,000 thermal shocks from -40°C to 110°C, with every joint conductive. The talk attributes this to a true metallurgical solder joint formed by diffusion and a classic Cu6Sn5 intermetallic about 2.5 micrometers thick, and extends low-temperature bismuth-tin soldering to rigid components on PET silver traces at 110°C.

About the speaker:
* Speaker: Ian Tevis
* Company: SAFI-Tech
* Event: Printed, Hybrid, InMold, and 3D Electronics
* Location: Online

#SAC305, #ThermalShockCycling, #BismuthTinSolder, #IntermetallicGrowth, #PrintedElectronics, #FlexibleElectronics


About this talk

→ Bringing performance of SAC solder to low temperature substrates · Ian Tevis · Printed, Hybrid, InMold, and 3D Electronics 2022


Other talks by Ian Tevis


More highlights from Ian Tevis

More Snippets
CONTACT US

KGH Concepts GmbH

Mergenthalerallee 73-75, 65760, Eschborn

+49 17661704139

admin@techblick.com

TechBlick is owned and operated by KGH Concepts GmbH

Registration number HRB 121362

VAT number: DE 337022439

  • LinkedIn
  • YouTube

Sign up for our newsletter to receive updates on our latest speakers and events AND to receive analyst-written summaries of the key talks and happenings in our events.

Thanks for submitting!

© 2026 by KGH Concepts GmbH