Christopher Tabor | US Department of Defense: How does a ~3 nm oxide shell govern liquid-metal particle stiffness, rupture, and coalescence on demand?
05:47 - 07:47
Other snippets from this talk
Summary of the clip:
How does a ~3 nm oxide shell govern liquid-metal particle stiffness, rupture, and coalescence on demand?
The effort began with fundamentals of oxide growth and thickness control. Colloidal suspensions are made by placing bulk liquid metal in solvent and sonicating or shear mixing; this top-down process breaks particles into smaller colloids. Size dispersion is controlled by agitation power and duration. Without control, the oxide grows to about three nanometers, and the work asks whether that growth can be made thinner or thicker during particle formation.
Oxide thickness has mechanical consequences. In situ SEM compression testing uses a nanoindentation tip to compress particles and compare mechanics and rupture under different loads according to shell thickness. A thinner oxide gives lower stiffness; a thicker oxide can be increased by changing how the shell grows on the particle outside. This provides a tool set for controlling how particles rupture.
The particles are described as little liquid-metal water balloons: individually they are not conductive because of the oxide shell. If two particles are placed next to each other, that shell blocks conduction. Rupturing them on demand allows individual particles to coalesce. The process that happens with silver during heating or photothermal heating can then happen with liquid-metal particles.
In this short video, you can learn:
* Uncontrolled oxide growth on liquid-metal colloids reaches about 3 nm.
* Nanoindentation in SEM shows oxide thickness changes particle stiffness and rupture load.
* Rupturing the oxide shell on demand enables nonconductive particles to coalesce.
📋 **Clip Abstract** Colloidal liquid-metal particles are produced top-down by sonication or shear mixing in solvent, with size dispersion set by agitation power and time. The native oxide is about 3 nm unless controlled; in situ SEM compression shows thinner shells lower stiffness and thicker shells alter rupture, and on-demand rupture lets isolated nonconductive particles coalesce.
About the speaker:
* Speaker: Christopher Tabor
* Company: US Department of Defense
* Event: Electronic Textiles & Skin Patches: Hardware & Software 2023
* Location: Online
#LiquidMetalColloids, #OxideShellThickness, #InSituSEMCompression, #RuptureOnDemand, #FlexibleElectronics, #ElectronicTextiles
This is a highlight of the presentation:
The Full Spectrum of Materials & Manufacturing Components Dedicated to the Digitization of the Materials’ Life Cycle
More Highlights from the same talk.
10:55 - 12:38
Can a stretchable conductor survive 10,000 cycles and 300–400% strain with almost no resistance change?
Can a stretchable conductor survive 10,000 cycles and 300–400% strain with almost no resistance change?
A simple PPU substrate hosts a connected particle network that does not immediately conduct — the particles stay individual, merely chemically linked. Applying mechanical force to the substrate, stretch or bend, transduces into that particle network. Each particle pulls on its neighbours, and that tension ruptures them, creating a conductive trace across the network. The process is non-reversible: once triggered, liquid pulls out of each particle and connects to its neighbour.
The resulting trace has been operated up to 10,000 cycles. The striking property is that the connectivity is very tortuous throughout the particle system, so the resistance is largely independent of strain: stretching to 300–400% produces almost no change in resistance between the two leads. Tortuosity manifesting throughout the network delivers the strain tolerance.
The mechanical picture resembles a coiled telephone cable: as you stretch it, it simply uncoils, but at the micron level. That makes the film a really bad strain sensor and a really good tool — a route to strain-tolerant circuitry whose properties do not shift as it is stretched, useful for stretchable conductors rather than for measuring deformation.
In this short video, you can learn:
* Mechanical force applied to a PPU substrate ruptures chemically linked particles into a non-reversible conductive trace.
* Activated traces have been cycled up to 10,000 times and hold resistance nearly constant out to 300–400% strain.
* Micron-scale tortuosity, likened to a coiled telephone cable, makes the network strain-tolerant and a poor strain sensor.
📋 **Clip Abstract** Stretch-activated particle networks on PPU substrates convert mechanical force into a non-reversible conductive trace by rupturing chemically linked particles. Because the resulting connectivity is tortuous at the micron level, the trace survives 10,000 cycles and 300–400% strain with almost no resistance change, making it a strain-tolerant conductor rather than a strain sensor.
About the speaker:
* Speaker: Christopher Tabor
* Company: US Department of Defense
* Event: Electronic Textiles & Skin Patches: Hardware & Software 2023
* Location: Online
#ParticleRuptureActivation, #StrainIndependentResistance, #PPUSubstrate, #StretchableCircuitry, #StretchableElectronics, #ElectronicTextiles
00:01:10.590 - 00:02:32.280
How can a three-nanometer oxide skin fundamentally override the capillary forces of a liquid metal alloy?
Can a three-nanometer oxide skin redefine the mechanical limits of liquid phase electronics?
The material science of gallium-based alloys presents a unique paradox where surface oxidation, typically viewed as a defect, becomes a critical structural enabler. On the very surface of these metals, a self-limiting three-nanometer oxide skin forms, imparting a level of mechanical stability that is entirely absent in conventional liquids. While standard liquids conform strictly to the volume of their container, this ultra-thin oxide shell allows the liquid metal to retain complex, freestanding geometries even when the oxide is selectively removed in specific regions.
Controlling this surface oxide opens up new pathways for developing drop-in replacements for stretchable conductive inks. By substituting traditional silver-based inks with a colloidal suspension of liquid metal particles, manufacturers can leverage existing printing infrastructures to produce highly compliant circuits. This approach transitions the unique rheological properties of gallium alloys from bulk demonstrations down to the nanoscale, offering a robust alternative to rigid particulate networks.
In situ characterization reveals the internal physical state of these sub-micron liquid metal particles under mechanical stress. When compressed under a 15-micron tip inside a scanning electron microscope (SEM), the particles demonstrate a highly ductile, "gooey" interior. As the protective oxide shell is crushed, the material deforms dynamically, forming intricate stalactite and stalagmite structures that highlight its fluid yet cohesive nature under localized deformation.
In this short video, you can learn:
* How a three-nanometer surface oxide skin provides mechanical stability to liquid gallium alloys.
* The potential of liquid metal colloidal suspensions as drop-in replacements for stretchable silver inks.
* How liquid metal particles behave under compression inside a scanning electron microscope.
📋 **Clip Abstract** The speaker discusses the material science of gallium-based alloys, focusing on how a three-nanometer surface oxide skin provides mechanical stability and allows liquid structures to retain their shape. He also explains how these liquid metal particles can serve as drop-in replacements for stretchable conductive inks, demonstrating their ductile behavior under SEM compression.
🎤 Speaker: Christopher Tabor
🏢 Company: Air Force Research Laboratory
📅 Event: Future of Electronics RESHAPED USA 2026
📍 Location: Computer History Museum, Mountain View, California, USA
🌐 Learn more at the next TechBlick event: https://www.techblick.com
#EGaIn, #LiquidMetal, #GalliumOxide, #MicroCompression, #StretchableElectronics, #PrintedElectronics
17:07 - 18:46
Can a liquid-metal coax cable be cut in half, reconnected, and keep its signal while stretched 400–500%?
Can a liquid-metal coax cable be cut in half, reconnected, and keep its signal while stretched 400–500%?
The clip shows a stretchable coaxial cable made from these element materials, with yellow and blue waveforms tracked as the cable is stretched. Across that stretch, the signals do not degrade and maintain their phase behavior: no changes are seen in the signal while the b and c coax cable is being stretched. The demonstration tracks those waveforms during stretching.
When the same cable is cut in half, the signal goes away, as expected. The substrate is tacky, so the two pieces can be brought back together and the system self-heals to regain signal quality across the liquid metal. The substrate must do that, and because the liquid metal is liquid, it reemerges and reconnects as the pieces meet.
The concept is used for data integration: a blue shirt carries a camera, and camera microphones can use integrated cabling so nothing hangs off the soldier. These cables stretch 400–500% without signal loss. In the lower video, the cable is strained while video is carried across it; if the cable broke, the signal would be lost and no video would arrive, so the setup watches itself being tortured.
In this short video, you can learn:
* Stretching the liquid-metal coaxial cable does not degrade the signal; phase behavior is maintained.
* A cut cable loses signal, but a tacky substrate plus liquid metal lets the two halves self-heal and regain signal quality.
* The cable withstands 400–500% stretch without signal loss and can carry video while being strained.
📋 **Clip Abstract** A stretchable coaxial cable made from element materials maintains signal phase as it is stretched, and it can be cut in half and self-healed by bringing the tacky substrate and liquid metal back together. The same integrated cabling concept stretches 400–500% without signal loss and carries video even while being strained.
About the speaker:
* Speaker: Christopher Tabor
* Company: US Department of Defense
* Event: Electronic Textiles & Skin Patches: Hardware & Software 2023
* Location: Online
#LiquidMetalCoax, #SelfHealingSubstrate, #StretchableCabling, #SignalPhaseStability, #ElectronicTextiles, #WearableElectronics
About this talk
→ The Full Spectrum of Materials & Manufacturing Components Dedicated to the Digitization of the Materials’ Life Cycle · Christopher Tabor · Electronic Textiles & Skin Patches: Hardware & Software 2023
Other talks by Christopher Tabor
- Resilient Packaging of Stretchable Electronics · Wearables RESHAPED USA 2026
- Liquid Metal Inks for Printed Stretchable Electronics · The Future of Electronics RESHAPED 2024 Berlin
More highlights from Christopher Tabor
- ▶ How can a three-nanometer oxide skin fundamentally override the capillary forces of a liquid metal alloy? · Future of Electronics RESHAPED USA 2026
- ▶ Why are printed liquid metal inks initially insulating, and how can stretching them make them conductive? · Future of Electronics RESHAPED USA 2026
- ▶ How can we achieve high moisture-vapor breathability in liquid metal skin-contact bioelectrodes? · Future of Electronics RESHAPED USA 2026
- ▶ How can a liquid metal have a solid structure? · The Future of Electronics RESHAPED 2024
- ▶ Can you create a conductive ink that only turns on when you stretch it? · The Future of Electronics RESHAPED 2024
- ▶ What happens to a video signal when you stretch the cable it's running through? · The Future of Electronics RESHAPED 2024