Mike Mastropietro | ACI Materials: If the ink costs more per kilogram, how can it lower the cost of a finished circuit?

13:40 - 15:23

Other snippets from this talk

Summary of the clip:

If the ink costs more per kilogram, how can it lower the cost of a finished circuit?

The inks can be formulated solvent-free as water-based systems. Although they cost more per kilogram than a traditional conductor, weight-based pricing is not the right comparison for a circuit. Designs target a resistance so the circuit functions, particularly in flexible hybrid electronics with active components. The relevant target is resistance over the traces between components, and the formulation’s solids and volume resistivity change the cost calculation.

The example uses a sheet resistance of 30 milliohms per square, described as the traditional polymer thick film upper limit of what was needed. Any number can be used. In some cases a design may need to achieve less, and polymer thick film cannot be used. The comparison therefore depends on the resistance target, not just the ink’s cost per kilo.

Because of superior solids and superior volume resistivity, the materials significantly reduce cost compared with a real competitive product that is not even known as one of the most expensive in the industry. Costs can actually be reduced using these materials. The clip then shows examples in use, with images courtesy of Chasm Technologies.

In this short video, you can learn:
* Water-based, solvent-free formulations are possible.
* The cost comparison must use the target resistance over traces between components, with 30 milliohms per square given as a traditional polymer thick film upper limit.
* Superior solids and volume resistivity can significantly reduce cost versus a competitive product not known as one of the most expensive in the industry.

📋 **Clip Abstract** The clip explains why a higher cost per kilogram can still lower finished-circuit cost: designs target resistance over traces between components, and the example uses 30 milliohms per square as a traditional polymer thick film upper limit. It attributes the cost reduction to superior solids and volume resistivity compared with a competitive product, and notes solvent-free water-based formulations and examples in use.

About the speaker:
* Speaker: Mike Mastropietro
* Company: ACI Materials
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online

Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/

#WaterBasedFormulations, #SheetResistance, #VolumeResistivity, #SolventFreeInk, #FlexibleHybridElectronics, #PrintedElectronics

This is a highlight of the presentation:

ACI Alchemy Conductive Inks -Enabling Next Generation Flexible & 3D Electronics

Printed, Hybrid, Structural & 3D Electronics 2021

​

11-12 May 2021

Online

Organised By:

TechBlick

​

More Highlights from the same talk.

02:34 - 05:04

Why combine microparticles and nanoparticles instead of choosing polymer thick film or sintering silver?

Why combine microparticles and nanoparticles instead of choosing polymer thick film or sintering silver?

Traditional polymer thick film silver conductors use conductive fillers in a thermoplastic polymer dissolved in solvent; drying forces particles together, but contact resistance remains. Their upside is good resin interface at the substrate, giving good adhesion, while electrical performance is at best maybe 10 times that of a bulk conductor such as silver or copper.

Sintering conductors differ: wet ink dries, particles come together, and thermal energy sinters them, avoiding the contact resistance seen with classic conductors. The challenge is getting resin to the interface without preventing sintering. These were the available classes for flexible hybrid electronics and printed electronics before ACI Alchemy conductive inks.

ACI Alchemy is described as a hybrid or semi-sintering conductor: microparticles like a traditional ink and nanoparticles like a sintering ink. This enables sintering while retaining resin at the interface, getting the best of both worlds. Traditional PTFE inks are about the resistivity of lead—about 19 microohm centimeters, or 15 milliohms per square per mil—while Alchemy targets polymer thick film ease, curing and process speed with much closer-to-precious-metal conductivity.

In this short video, you can learn:
* Polymer thick film silver inks offer good substrate adhesion but retain contact resistance and electrical performance at best maybe 10 times that of bulk silver or copper.
* Sintering inks reduce contact resistance through thermal particle sintering, yet resin must reach the interface without blocking sintering.
* ACI Alchemy combines microparticles and nanoparticles in a semi-sintering conductor to obtain sintering with resin at the interface, while aiming for polymer thick film process ease and closer-to-precious-metal conductivity.

📋 **Clip Abstract** Traditional polymer thick film conductors provide good adhesion but suffer contact resistance, while sintering inks avoid it but struggle to place resin at the interface without inhibiting sintering. ACI Alchemy uses microparticles plus nanoparticles in a hybrid semi-sintering conductor, pursuing sintering with resin at the interface and polymer thick film ease, curing and process speed with conductivity much closer to the precious metal.

About the speaker:
* Speaker: Mike Mastropietro
* Company: ACI Materials
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online

Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/

#PolymerThickFilm, #SinteringSilver, #MicroparticleNanoparticle, #ConductiveInks, #FlexibleHybridElectronics, #PrintedElectronics

22:23 - 24:44

Can silver inks survive rising silver prices against copper and graphene alternatives?

Can silver inks survive rising silver prices against copper and graphene alternatives?

The argument starts with graphene: its resistivity is cited as 1,000 times higher, while its cost is only a quarter to a tenth, so the speaker limits its printed-conductor role to being perfectly carbon-based. Silver is not defended in isolation; the comparison shifts to what an ink costs to make and process. Copper metal can be expensive, but ink economics depend on particle manufacturing and processing.

Copper inks carry two practical penalties. Processing with nitrogen firing or calendaring limits substrate choices and requires complex equipment, so the ink cannot simply run in existing dryers. A low-temperature nano copper ink may show ultimate performance that is only a hair better, but the stable-performance problem appears in temperature-humidity studies: copper oxidizes, and the thinner the film, the quicker it happens.

The oxidation percentage, which the speaker says can be found in the patents, means copper becomes more expensive over time for the same sheet resistance. That is the response to silver-price pressure: the cheaper ink is judged on processed cost and stable sheet resistance, not metal price alone. The speaker also notes both are heavy metals, closing that part of the comparison without endorsing a graphene swap.

In this short video, you can learn:
* Graphene inks are described as having 1,000 times higher resistivity while costing only a quarter to a tenth as much.
* Copper inks require nitrogen firing or calendaring, which limits substrates and demands complex equipment rather than existing dryers.
* Copper oxidation in temperature-humidity studies makes thinner films degrade faster and raises cost for the same sheet resistance over time.

📋 **Clip Abstract** Silver-price pressure is addressed by comparing graphene, copper and silver inks on resistivity, particle-processing cost and stable sheet resistance. Copper inks may be cheaper, but nitrogen firing, calendaring and oxidation make their processed cost and long-term sheet resistance the decisive measures.

About the speaker:
* Speaker: Mike Mastropietro
* Company: ACI Materials
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online

Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/

#SilverConductiveInk, #CopperInkOxidation, #NitrogenFiring, #SheetResistance, #PrintedElectronics, #FlexibleElectronics

07:38 - 09:24

How many creases can a printed silver trace survive if the film is made thinner?

How many creases can a printed silver trace survive if the film is made thinner?

Polymer thick film proponents have long argued that resin-free conductors cannot be creased, so the FlexTech award work set out to demonstrate mechanical ability. Traditional ASTM crease tests, where a weight is rolled over the sample, were passed easily — even after cracking, rolling the sample flat pushes the cracks back together. That prompted a dedicated tension-free U-Flex method run in a mode that crushes the sample like the crease test.

When resistance is logged continuously as the crease happens, the comparison is stark. A polymer thick film ink — a very good one, at about 8 milliohms per square per mil volume resistivity with a good balance of resolution and flexibility — breaks on the first crease, shown in red. The Alchemy series ink survives until the fourth crease before it starts to break.

Copper foil suppliers frame crease failure as a function of substrate thickness and film thickness, and that explanation holds. Because the same sheet resistance is reached at a much thinner film thickness, survivability improves. Flex ductility, not shown in the crease data, was also tested with these materials and performed excellently, so the mechanical performance claim rests on more than one measurement.

In this short video, you can learn:
* Because rolling a cracked sample flat pushes the cracks back together, traditional ASTM crease tests understate damage, which is why a tension-free U-Flex crush mode was developed.
* The polymer thick film ink at roughly 8 milliohms per square per mil volume resistivity broke on the first logged crease, while the Alchemy series ink only began breaking on the fourth.
* Reaching the same sheet resistance at a much thinner film thickness is what drives crease survivability, and the same materials also performed excellently in flex ductility testing.

📋 **Clip Abstract** Continuous resistance logging during a crushing crease test separates a polymer thick film ink, which fails on the first crease, from an Alchemy series ink that survives to the fourth. The gain is attributed to achieving the same sheet resistance at a much thinner film, with flex ductility also confirmed.

About the speaker:
* Speaker: Mike Mastropietro
* Company: ACI Materials
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online

Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/

#ConductiveInk, #CreaseTesting, #SheetResistance, #FlexDuctility, #FlexibleElectronics, #PrintedElectronics


About this talk

→ ACI Alchemy Conductive Inks -Enabling Next Generation Flexible & 3D Electronics · Mike Mastropietro · Printed, Hybrid, Structural, & 3D Electronics 2021

More Snippets
CONTACT US

KGH Concepts GmbH

Mergenthalerallee 73-75, 65760, Eschborn

+49 17661704139

admin@techblick.com

TechBlick is owned and operated by KGH Concepts GmbH

Registration number HRB 121362

VAT number: DE 337022439

  • LinkedIn
  • YouTube

Sign up for our newsletter to receive updates on our latest speakers and events AND to receive analyst-written summaries of the key talks and happenings in our events.

Thanks for submitting!

© 2026 by KGH Concepts GmbH

bottom of page