top of page

Reed Eisenhart

Phillips 66

* All members of the platform can watch the entire presentation.

 

Please register to become a member.

Reed Eisenhart | Phillips 66: Why does a TRMC-measured carrier diffusion length predict the 250 nm optimum thickness that large-area printing needs?

07:25 - 09:51

Other snippets from this talk

Summary of the clip:

Why does a TRMC-measured carrier diffusion length predict the 250 nm optimum thickness that large-area printing needs?

TRMC screening of OPV blends shows a clear correlation: materials predicted to have very long free-charge-carrier diffusion lengths, plotted on the x-axis, reach maximum PCE at thicker films. The cluster with shorter TRMC diffusion lengths follows the standard profile, peaking at 100–150 nm. The long-diffusion materials instead maximize PCE near 250 nm, the thickness targeted for large-area coating.

One polymer, P77, was slot-die coated into thick active layers, including a very thick film labeled N, while retaining high performance and supporting defect-free large-area coating. Small-area P77 devices in red increased from 200 to 300 to 400 nm without a PCE drop-off. Slot-die-coated cells in green also showed no efficiency drop from 200 to 400 nm, though efficiencies were lower—about 8%, not 10%.

This contrasts with common literature polymers that publish high performance at 100 nm but drop off quickly at higher thicknesses. P77’s flat thickness response means coating variability from 200 to 400 nm still yields stable performance, which the speaker calls a big enabler for large-area printing. The second challenge being tackled is scalable coating, where the question is asked.

In this short video, you can learn:
* TRMC-predicted long free-charge-carrier diffusion lengths correlate with maximum PCE at about 250 nm rather than 100–150 nm.
* P77 small-area and slot-die-coated devices retained stable PCE from 200 to 400 nm, with slot-die efficiencies around 8%.
* Literature polymers peaking at 100 nm drop off quickly at higher thickness, whereas P77’s flat response supports large-area coating variability.

📋 **Clip Abstract** TRMC screening links longer free-charge-carrier diffusion lengths to OPV active layers that maximize PCE near 250 nm, the thickness needed for large-area coating. P77 retains stable performance from 200 to 400 nm in small-area and slot-die-coated cells, contrasting with literature polymers that drop off beyond 100 nm.

About the speaker:
* Speaker: Reed Eisenhart
* Company: Phillips 66
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online

Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/

#TRMCScreening, #SlotDieCoatedOPV, #P77Polymer, #ThicknessStablePCE, #OrganicPhotovoltaics, #LargeAreaPrinting

This is a highlight of the presentation:

Photoactive Polymers Tailored to Industrial Printing of High Performing and Stable Organic Photovoltaics

Printed, Hybrid, Structural & 3D Electronics 2021

​

11-12 May 2021

Online

Organised By:

TechBlick

​

More Highlights from the same talk.

12:58 - 14:37

Why did a 12% world-record OPV active layer fail completely when slot-die coated, and what fixed it?

Why did a 12% world-record OPV active layer fail completely when slot-die coated, and what fixed it?

Spin-coated results are a poor predictor of large-area performance. A 2017 world-record active layer exceeded 12% efficiency with PCBM in spin-coated cells, but scaling to slot-die coating produced too much PCBM aggregation, defects and shorts — workable devices could not be made at all. Switching from PCBM to non-fullerene acceptors improved coating, yet performance still dropped sharply. The first lesson: active layers must be designed for large-area printing processes.

The response was new materials, including P77, which reached over 10% PCE with PCBM when spin-coated. That translated only decently to slot die — 4% PCE — because PCBM is genuinely hard to slot-die coat. P77 was designed with high viscosity that suppressed acceptor aggregation and gave nice films with PCBM.

Even better, replacing PCBM with a non-fullerene acceptor allowed slot-die coating of stripes at 8% PCE on 3 cm² device sizes. That is a strong result for large-area slot-die coated OPV active layers, and it shows how material design, not just process tuning, decides whether a record cell survives the transition to printing.

In this short video, you can learn:
* A 2017 world-record active layer above 12% spin-coated efficiency could not be turned into workable devices by slot-die coating because of PCBM aggregation, defects and shorts.
* Non-fullerene acceptors gave better coating than PCBM but performance still fell, until materials such as P77 were designed with high viscosity to prevent acceptor aggregation.
* P77 with a non-fullerene acceptor reached 8% PCE in slot-die coated stripes on 3 cm² devices, far above the 4% obtained with PCBM.

📋 **Clip Abstract** Spin-coated champion efficiencies do not transfer reliably to large-area slot-die coating, as a 12% PCBM-based world-record active layer that aggregated, shorted and yielded no workable devices showed. Redesigning the polymer for printing — high-viscosity P77 with a non-fullerene acceptor — delivered 8% PCE in slot-die coated stripes on 3 cm² devices.

About the speaker:
* Speaker: Reed Eisenhart
* Company: Phillips 66
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online

Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/

#SlotDieCoating, #PCBMAggregation, #NonFullereneAcceptor, #LargeAreaOPV, #OrganicPhotovoltaics, #PrintedElectronics

14:37 - 16:53

Which industrial constraints—green solvents, fast drying, low temperatures, solution interlayers—flip the ranking of two polymers?

Which industrial constraints—green solvents, fast drying, low temperatures, solution interlayers—flip the ranking of two polymers?

Large-area slot-die-coated OPV active layers reached a nice PCE, and pilot evaluation tracked air stability, uniform films and morphology control using scalable processes. The industrial constraints were explicit: reduced-toxicity formulations replacing halogenated solvents, very fast drying because the film must dry before hitting a roller, and lower temperatures. Literature anneals of 110–150 °C may help morphology but cannot work on plastic substrates.

Slot-die coating cannot heat solvents to 100 °C during coating, adding temperature constraints. Compatible solution-processed layers are also required: lab cells often evaporate molybdenum oxide as the whole transport layer, but that is not viable over large areas. The material set must therefore tolerate interlayers coated from solution on top. These are the process realities that laboratory performance alone does not capture.

In lab-scale slot-die coating in air with chlorobenzene, polymer A (P77) gave 8% and polymer B 7.6%. Originally polymer A would have been called more promising. Moving to a green, non-halogenated solvent blend reversed that: polymer B was much superior, while polymer A only decreased. This is how materials are put through their paces to see which are really more promising.

In this short video, you can learn:
* Pilot evaluation required air-stable materials, uniform films and controllable morphology using scalable processes.
* Industrial printing imposes fast drying before rollers, low temperatures instead of 110–150 °C anneals, and solution-processed interlayers compatible with large areas.
* In air, lab-scale slot-die coatings with chlorobenzene gave P77 8% and polymer B 7.6%, but a green non-halogenated blend made polymer B much superior.

📋 **Clip Abstract** Pilot evaluation of large-area slot-die-coated OPV active layers focused on air stability, uniform films and morphology control under scalable processing. Industrial constraints—halogenated solvent replacement, fast drying before rollers, low-temperature processing and solution-processed interlayers—reversed the lab ranking: with chlorobenzene P77 reached 8% and polymer B 7.6%, but in a green non-halogenated blend polymer B was much superior.

About the speaker:
* Speaker: Reed Eisenhart
* Company: Phillips 66
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online

Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/

#SlotDieCoating, #NonHalogenatedSolvents, #OPVActiveLayers, #SolutionProcessedInterlayers, #OrganicPhotovoltaics, #PrintedElectronics


About this talk

→ Photoactive Polymers Tailored to Industrial Printing of High Performing and Stable Organic Photovoltaics · Reed Eisenhart · The Future of Photovoltaics: Organic, Perovskites, CIGS, Hybrid 2021


Other talks by Reed Eisenhart

More Snippets
CONTACT US

KGH Concepts GmbH

Mergenthalerallee 73-75, 65760, Eschborn

+49 17661704139

admin@techblick.com

TechBlick is owned and operated by KGH Concepts GmbH

Registration number HRB 121362

VAT number: DE 337022439

  • LinkedIn
  • YouTube

Sign up for our newsletter to receive updates on our latest speakers and events AND to receive analyst-written summaries of the key talks and happenings in our events.

Thanks for submitting!

© 2026 by KGH Concepts GmbH

bottom of page