Ryan Banfield | Heraeus Electronics: Why is a solderable polymer necessary when high-temperature fired materials have been available for decades?
00:00:45 - 00:00:47
Other snippets from this talk
Summary of the clip:
Why is a solderable polymer necessary when high-temperature fired materials have been available for decades?
The speaker introduces the concept of a solderable polymer material and poses the question of its necessity, given the existing high-temperature fired materials. He highlights his extensive experience in the printed electronics industry, spanning approximately 25 years. He notes that since the advent of the membrane switch in the mid-1970s, the industry has been aiming to replace traditional subtractive technology.
However, the speaker argues that the focus should shift from replacement to augmentation and support. He suggests leveraging the knowledge and advancements from the traditional technology industry and integrating them into the printed electronics sector. The core limitation of the polymer thick film industry, according to the speaker, lies in solderability.
The ability to attach components directly to the substrate has been restricted to two-part or one-part epoxy-based materials, which present challenges such as long pot life, viscosity changes over time, evolving processing parameters, extended cure cycles, and low attachment rates. The speaker asserts that solder, in every aspect, is superior to epoxy-based materials due to its snap cure, higher conductivity, enhanced mechanical strength, and improved reliability in demanding applications.
In this short video, you can learn:
* The historical context of printed electronics and its relationship with subtractive technologies.
* The limitations of epoxy-based materials in printed electronics applications.
* The advantages of solder over epoxy in terms of performance and reliability.
📋 **Clip Abstract:** This segment introduces the need for solderable polymers by contrasting them with existing solutions like epoxies and high-temperature materials, highlighting the limitations of current approaches in printed electronics. It sets the stage for understanding the benefits of the new material.
🔗 Link in comments 👇
#SolderablePolymer, #PolymerThickFilm, #ComponentAttachment, #EpoxyAdhesives, #PrintedElectronics, #ElectronicPackaging
This is a highlight of the presentation:
Bridging the Gap Between Additive and Subtractive Technologies: the Solderable Polymer Revolution.
More Highlights from the same talk.
04:00 - 05:47
Does a printed ink turning dark after a 300 °C ramp mean it has lost conductivity?
Does a printed ink turning dark after a 300 °C ramp mean it has lost conductivity?
Two discs were run in thermogravimetric analysis or DSC instrumentation. One measures weight loss, one measures energy given or taken by the material. The samples were two mainstay inks in the polymer thick film portfolio of the Heraeus Prylex group, the thick film low temperature line. They were ramped to 300 °C for ten minutes after a 30 °C burn-off of the solvents.
The two materials showed a vast color difference. The cracking on the left is due to pooling of material on the edge, not temperature; that is mud cracking seen if a print is too thick. Color is not always a huge indicator that the material does not function properly.
These are functional electronic printers, not graphic printers, so the main concerns are whether the ink is conductive, whether it works, and whether it sticks to the end of the life of the application. Storage data shown was ink taken up to 250 °C for 30 minutes and held.
In this short video, you can learn:
* The Heraeus Prylex polymer thick film inks were ramped to 300 °C for ten minutes after a 30 °C solvent burn-off.
* Mud cracking came from material pooling at the edge and too thick a print, not from the temperature.
* Functional electronic printing prioritizes conductivity, function, and adhesion over color, with storage data at 250 °C for 30 minutes.
📋 **Clip Abstract** Two mainstay polymer thick film inks from the Heraeus Prylex group were compared after a 300 °C, ten-minute ramp following a 30 °C solvent burn-off. Color differed vastly, but the cracking was mud cracking from pooling and thick printing, and functional electronic printing cares about conductivity, function, and adhesion, with storage data at 250 °C for 30 minutes.
About the speaker:
* Speaker: Ryan Banfield
* Company: Heraeus Electronics
* Event: nnovation Festival: Additive, Printed, Sustainable Electronics, MicroLEDs and AR/VR Displays, Perovskites | July 2026
* Location: Online Platform
Annual access to our onsite event(s), all online events and a library featuring over 1800 presentations (recordings + PDF) across all our onsite and onsite events and technology areas. Join us and over 2000 members from around the world now.
Explore and join now --> https://www.techblick.com/
#PolymerThickFilm, #ThermogravimetricAnalysis, #SolventBurnOff, #MudCracking, #PrintedElectronics, #AdditiveElectronics
03:20 - 04:46
How much does trace geometry — not the ink — change measured stretchability, and by what factor?
How much does trace geometry — not the ink — change measured stretchability, and by what factor?
Stretchability needs definition: a customer may mean 300% once or 10% a million times. The test printed the same pattern at three widths and stretched it in two directions. That distinction frames how design choices affect one-time stretch versus repeated stretch, because “stretchability” alone does not specify the strain mode or cycle count.
In longitudinal testing, the serpentine trace is not printed in a straight line, so force is applied over a much smaller area as the trace stretches out. The longitudinal stress result showed an increase of about a factor of four or five times, and it was pretty even across all the traces tested.
Switching to lateral testing produced a much larger increase because the path has less of the S shape associated with the serpentine route. The takeaway is that trace geometry can change measured stretchability; design considerations matter exponentially when establishing what stretchability means for an application. The same pattern and three widths isolate that geometry effect.
In this short video, you can learn:
* The clip distinguishes 300% stretch once from 10% stretch a million times as different definitions of stretchability.
* Longitudinal serpentine testing raised stress by about four or five times, fairly evenly across three printed widths.
* Lateral testing gave a much larger increase because the trace path had less of the serpentine S shape.
📋 **Clip Abstract** This clip shows that stretchability must be defined by strain level and cycle count, not by a single label. Using the same pattern at three widths, longitudinal serpentine traces increased stress about four or five times, while lateral testing produced a much larger increase because the path had less S shape.
About the speaker:
* Speaker: Ryan Banfield
* Company: Heraeus Electronics
* Event: Electronics RESHAPED 2026 | Berlin
* Location: Estrel, Berlin
USA: The Future of Electronics RESHAPED | USA
📅 Save the date: 9 and 10 June 2027
📍 Mountain View, California (Silicon Valley)
📋 Info: https://www.techblick.com/electronicsreshapedusa
Europe
The Future of Electronics RESHAPED | Berlin
📅 Save the date: 20 and 21 October 2027
📍 Berlin, Germany
📋 Info: https://www.techblick.com/electronicsreshaped
#SerpentineTraceGeometry, #LongitudinalStretchTesting, #LateralStretchTesting, #TraceWidthTestPattern, #StretchableElectronics, #PrintedElectronics
08:46 - 10:29
Are percent-shifted datasheet resistance figures correlative, and why does short-term high temperature demand polyimide over PET?
Are percent-shifted datasheet resistance figures correlative, and why does short-term high temperature demand polyimide over PET?
Technical datasheets and product presentations often contain what amounts to magic hand-waving: moving from ohm per square per mil, a normalized figure, to percent, in ways that are not correlative to your own data. The presented work instead aims to show results that correlate directly to the application being targeted, rather than a normalized number that travels badly.
Post-crease resistance change was measured to show that adhesion did not change for either material; the post-crease resistances were very similar across the high temperature exposure tested. The ASTM testing itself was not covered, and more data remains to be shared, so treat this as an indication rather than the complete dataset.
There is a common industry habit of using whatever is at hand, which invites forcing a familiar material into an application, wrenches used as hammers. Everybody uses PET because the cost is there, but high temperature stability, even short term, requires a polyimide-type substrate. Right tool, right job.
In this short video, you can learn:
* Datasheet conversions from ohm per square per mil to percent are not necessarily correlative to an application's real data.
* A crease test showed no adhesion change for either material, with post-crease resistances very similar across the high temperature exposure.
* Short-term high temperature stability still requires a polyimide substrate rather than PET, despite PET's lower cost.
📋 **Clip Abstract** Datasheets that convert normalized ohm per square per mil values into percentages risk presenting figures that are not correlative to the target application. Crease testing showed unchanged adhesion, and the substrate message is blunt: high temperature duty, even short term, belongs on polyimide, not PET chosen for cost.
About the speaker:
* Speaker: Ryan Banfield
* Company: Heraeus Electronics
* Event: nnovation Festival: Additive, Printed, Sustainable Electronics, MicroLEDs and AR/VR Displays, Perovskites | July 2026
* Location: Online Platform
Annual access to our onsite event(s), all online events and a library featuring over 1800 presentations (recordings + PDF) across all our onsite and onsite events and technology areas. Join us and over 2000 members from around the world now.
Explore and join now --> https://www.techblick.com/
#SheetResistanceData, #CreaseTesting, #PolyimideSubstrates, #PETSubstrates, #FlexibleElectronics, #PrintedElectronics
About this talk
→ Bridging the Gap Between Additive and Subtractive Technologies: the Solderable Polymer Revolution. · Ryan Banfield · The Future of Electronics RESHAPED 2025
Other talks by Ryan Banfield
- AG Inks for Stretchable Electronics: A continuance · The Future of Electronics RESHAPED 2026 Berlin
- Ag Inks for Stretchable Electronics · TechBlick Innovations Festival July 2026
- Limitations of future wearable/medical trends and their development hurdles: A paste supplier’s perspective · The Future of Electronics RESHAPED 2025 USA
- Functional electronic inks as an enabler for the latest advancements in healthcare · The Future of Electronics RESHAPED 2024 USA
More highlights from Ryan Banfield
- ▶ How much does trace geometry — not the ink — change measured stretchability, and by what factor? · Electronics RESHAPED 2026 | Berlin
- ▶ Why do wearable electronics market reports disagree so wildly on base-year market value? · Electronics RESHAPED 2026 | Berlin
- ▶ Can laminating a second substrate on top double your stretchable circuit's elongation and lifetime? · Electronics RESHAPED 2026 | Berlin
- ▶ Which stretchable electronics market is in production today, and which one takes over next? · Electronics RESHAPED 2026 | Berlin
- ▶ Does a printed ink turning dark after a 300 °C ramp mean it has lost conductivity? · Innovation Festival: Additive, Printed, Sustainable Electronics
- ▶ Are percent-shifted datasheet resistance figures correlative, and why does short-term high temperature demand polyimide over PET? · Innovation Festival: Additive, Printed, Sustainable Electronics
- ▶ How does the solvent system contribute to the functionality of silver chloride ink? · The Future of Electronics RESHAPED USA | Boston 2025
- ▶ What are the primary challenges in achieving stretchable electronics with silver chloride inks? · The Future of Electronics RESHAPED USA | Boston 2025
- ▶ Why is collaboration between ink manufacturers and end-users crucial for optimizing silver chloride ink formulations? · The Future of Electronics RESHAPED USA | Boston 2025