Stefan Bergfeld | Bergfeld Lasertech: Which laser parameters really matter when developing selective material removal across lab and production?
18:46 - 20:23
Other snippets from this talk
Summary of the clip:
Which laser parameters really matter when developing selective material removal across lab and production?
In laser selective material processing, laboratory systems expose far more variables than production: scan speed and pulse repetition rate, but also wavelength, fluency, power, pulse energy independent of power, increment, number of passes and relay lengths. That breadth lets researchers control everything they want, yet production cannot replicate it. The parameter space itself becomes the experimental challenge.
Picosecond burst mode can make the process very complex, and scan strategy depends on the fume extraction being used. Working off focus, in focus or around can be challenging, especially for material scientists who are not laser specialists. Those choices interact with the many controllable laser parameters, so selective removal is not just a single pulse-energy setting.
Training is offered to close that gap: a training lab in Aachen holds all the lasers, and teaching covers the system controls. A small, cheap SEM adds electroluminescence and photoluminescence, and this module can be implemented into other systems. The aim is to train material scientists on the parameters and strategies that selective laser processing actually requires.
In this short video, you can learn:
* Laboratory laser systems expose wavelength, fluency, independent pulse energy, increment, pass count and relay length as controllable variables.
* Picosecond burst mode and fume-extraction-dependent scan strategy complicate selective processing for non-laser material scientists.
* A small SEM with electroluminescence and photoluminescence can be added as a module and supported by training in Aachen.
📋 **Clip Abstract** Selective laser material processing in the lab exposes parameters that production cannot match, including wavelength, fluency, independent pulse energy, increment, passes and relay lengths. Picosecond burst mode, fume-extraction-dependent scan strategy and focus position add complexity, so training and SEM-based electroluminescence/photoluminescence modules support material scientists.
About the speaker:
* Speaker: Stefan Bergfeld
* Company: Bergfeld Lasertech
* Event: Perovskite Connect 2026 | Berlin
* Location: Estrel, Berlin
Save the date: Perovskite Connect 2027 | 20 and 21 OCT 2027 | Berlin
Co-located with the Future of Electronics RESHAPED conference and exhibition
Learn more: https://www.techblick.com/perovskiteconnect
Intestered in exhibiting: learn more here: https://www.techblick.com/perovskiteconnect
#LaserSelectiveProcessing, #PicosecondBurstMode, #FumeExtractionScanStrategy, #ElectroluminescencePhotoluminescenceSEM, #PerovskitePV, #LaserMaterialProcessing
This is a highlight of the presentation:
New laser platform for research and pilot production enables opportunities in perovskite PV.
21 and 22 OCT 2026
Estrel, Berlin
Organised By:
More Highlights from the same talk.
02:47 - 05:06
Does film-side versus glass-side ablation change perovskite P3 fluence and process-speed windows?
Does film-side versus glass-side ablation change perovskite P3 fluence and process-speed windows?
The clip compares ITO-on-glass with the substrate turned around: left is film-side ablation, right is substrate-side ablation. The surface electrical fields are opposite because of refractive-index change, so the two cases look different in simulation. Both routes work, and when the substrate is transparent, both are available; users choose either film-side or substrate-side processing.
For perovskite/ITO/glass, a 10 picosecond laser shows different temperature profiles. From the glass side, heating occurs directly at the surface, maybe within 100 nanometers. From the film side, the pulse hits perovskite directly and ablates layer by layer. Both work, but process speed and fluences—energy density—are quite different, so the choice can be an advantage or disadvantage.
From the glass side, one pulse can erase everything; from the film side, you need to dig through pulses. For P3, erasing perovskite under a metal back contact can produce flakes even with short pulses, so P3 may be done from the film side. Adding a hole transport layer can change these possibilities, making flexibility important.
In this short video, you can learn:
* Film-side and substrate-side ablation both work on transparent substrates, but opposite surface fields and refractive-index change alter the process.
* With a 10 picosecond laser, glass-side processing heats near the surface and can erase all layers in one pulse, while film-side processing ablates layer by layer.
* P3 scribing through perovskite with a metal back contact risks flakes even with short pulses, and a hole transport layer can change the available options.
📋 **Clip Abstract** The comparison turns an ITO-on-glass substrate around to contrast film-side and substrate-side ablation, showing opposite surface electrical fields from refractive-index change. Using a 10 picosecond laser on perovskite/ITO/glass, glass-side versus film-side processing differs in temperature profile, process speed and fluence, and P3 with a metal back contact can generate flakes even with short pulses.
About the speaker:
* Speaker: Stefan Bergfeld
* Company: Bergfeld Lasertech
* Event: Perovskite Connect 2026 | Berlin
* Location: Estrel, Berlin
Save the date: Perovskite Connect 2027 | 20 and 21 OCT 2027 | Berlin
Co-located with the Future of Electronics RESHAPED conference and exhibition
Learn more: https://www.techblick.com/perovskiteconnect
Intestered in exhibiting: learn more here: https://www.techblick.com/perovskiteconnect
#FilmSideAblation, #SubstrateSideAblation, #PicosecondLaser, #PerovskiteP3, #PerovskitePV, #LaserScribing
10:50 - 12:11
Can laser edge deletion scale at real speed while preserving perovskite module lifetime?
Can laser edge deletion scale at real speed while preserving perovskite module lifetime?
The platform spans long-picosecond and short-picosecond laser sources, each with three wavelengths. More than ten systems are running in the field—probably fifteen, though some are slightly different. Retrofit to glove boxes is usual, and systems have also been sent along; vacuum tracks are now being added to make foils. A laser-paper sheet demonstrates the setup, not a customer sample.
At real speed, laser edge deletion is shown at a factor of five using the weakest laser, and the result remains quite precise. The evacuation tunnel was removed from view, but evacuation is crucial: poor evacuation can mess up a lot of things. Alignment is handled in the system, and a tunnel usually surrounds the process.
There is discussion that laser scribing could affect the lifetime of the module. It is not clear from the talk, but that risk is flagged as something to consider. The demonstration uses the weakest laser, just to watch, with precision and evacuation as key process controls.
In this short video, you can learn:
* More than ten—probably fifteen—systems with three wavelengths are running in the field, spanning long- and short-picosecond sources.
* Laser edge deletion was demonstrated at a factor of five using the weakest laser, with alignment handled in the system.
* Evacuation is crucial because poor evacuation can mess up a lot, and laser scribing's effect on module lifetime is flagged but not confirmed.
📋 **Clip Abstract** A laser platform with long- and short-picosecond sources, three wavelengths and more than ten field systems is presented for research and pilot production. Laser edge deletion runs at a factor of five with the weakest laser, while evacuation and a possible scribing effect on module lifetime are flagged as process concerns.
About the speaker:
* Speaker: Stefan Bergfeld
* Company: Bergfeld Lasertech
* Event: Perovskite Connect 2026 | Berlin
* Location: Estrel, Berlin
Save the date: Perovskite Connect 2027 | 20 and 21 OCT 2027 | Berlin
Co-located with the Future of Electronics RESHAPED conference and exhibition
Learn more: https://www.techblick.com/perovskiteconnect
Intestered in exhibiting: learn more here: https://www.techblick.com/perovskiteconnect
#LaserEdgeDeletion, #PicosecondLaser, #ThreeWavelengthLaser, #GloveBoxRetrofit, #PerovskitePV, #SolarModuleLifetime
05:23 - 07:31
When do shorter laser pulses actually improve perovskite scribing, and when is pulse duration irrelevant?
When do shorter laser pulses actually improve perovskite scribing, and when is pulse duration irrelevant?
The pulse-duration decision starts with budget: shorter pulses if money allows, longer pulses to save it. But whether it matters is set by the perovskite's optical penetration depth, mapped against the system wavelengths — infrared, green, UV and deep UV, plus laser diodes. At infrared there is almost no absorption; in the green, absorption is fairly good, around 100 nm, or 50 to 200 nm measured precisely.
Plotting thermal diffusion lengths — for nanosecond pulses and for 10 picoseconds — against those penetration depths gives the answer. Where optical penetration depth is large, longer pulses are acceptable, because the beam reaches deep into the material anyway. Where the wavelength is short and penetration shallow, pulse duration really matters: 10 picoseconds delivers very precise ablation.
Perovskites differ from one another, and moving to UV tightens the precision further. The comparison holds only within linear parameters: femtosecond sources were deliberately left out because a further nonlinear absorption effect enters. Picosecond lasers are already in practical use, so the platform choice is really about matching penetration depth, diffusion length and budget rather than chasing the shortest pulse available.
In this short video, you can learn:
* Shorter pulses cost more and longer pulses save money, but pulse duration only becomes irrelevant when the perovskite's optical penetration depth is large enough.
* Infrared gives almost no absorption in perovskite, green gives roughly 100 nm penetration (50 to 200 nm measured precisely), and UV is more precise still.
* Femtosecond sources sit outside this linear comparison because a nonlinear absorption effect enters, while 10-picosecond pulses already deliver precise ablation.
📋 **Clip Abstract** Pulse duration is only a lever when optical penetration depth is shallow: infrared barely absorbs in perovskite, green sits near 100 nm, UV is shorter still. Placing those depths against nanosecond and 10-picosecond thermal diffusion lengths shows where longer pulses suffice and where short pulses buy precision.
About the speaker:
* Speaker: Stefan Bergfeld
* Company: Bergfeld Lasertech
* Event: Perovskite Connect 2026 | Berlin
* Location: Estrel, Berlin
Save the date: Perovskite Connect 2027 | 20 and 21 OCT 2027 | Berlin
Co-located with the Future of Electronics RESHAPED conference and exhibition
Learn more: https://www.techblick.com/perovskiteconnect
Intestered in exhibiting: learn more here: https://www.techblick.com/perovskiteconnect
#LaserScribing, #PulseDuration, #PerovskiteAblation, #UVWavelength, #ThinFilmPV, #PerovskitePV
About this talk