Ajay Virkar | C3Nano: Can one integrated hardcoat hold low surface energy and high contact angles through steel wool scratching?
13:40 - 14:49
Other snippets from this talk
Summary of the clip:
Can one integrated hardcoat hold low surface energy and high contact angles through steel wool scratching?
All the functions sit in the base coating itself. Unlike many commercial flexible hard coats on the market, no second anti-fingerprint coating or subsequent coating is required — and those added layers are typically very prone to being removed anyway. That integration is what the comparison set out to test.
The team bought a commercial flexible device already on the market, stripped off its flexible hard coat film and benchmarked it against ActiveGuard HC under standard steel wool scratch testing, measuring contact angles of several liquids before and after. The competitor shows visible scratches, surface energy rising dramatically and contact angles falling after the same harsh scratching.
Their film keeps very high contact angles after the same steel wool testing — even for a challenging liquid like hexadecane — evidence of a genuinely low surface energy substrate that survives harsh abrasion, rather than the surface energy climb seen on the incumbent. The product is now in the design-in phase.
In this short video, you can learn:
* Functions are built into the base hard coat so no separate anti-fingerprint layer is needed, removing a layer that is typically prone to removal.
* In steel wool scratch testing, the competitor's stripped-back commercial film showed visible scratches, rising surface energy and collapsing contact angles.
* ActiveGuard HC retained very high contact angles after the same scratching, including with hexadecane, and is in the design-in phase.
📋 **Clip Abstract** A commercial flexible device was stripped of its hard coat film and benchmarked against ActiveGuard HC under steel wool scratch testing, tracking contact angles of several liquids before and after. The integrated single-layer coating held high contact angles, including for hexadecane, while the competitor scratched visibly and saw surface energy rise.
About the speaker:
* Speaker: Ajay Virkar
* Company: C3Nano
* Event: Printed, Hybrid, Structural & 3D Electronics 2021
* Location: Online
Join TechBlick - the home of printed electronics, additive electronics, flexible hybrid electronics and 3D electronics
https://www.techblick.com/
#HardCoat, #SteelWoolScratch, #ContactAngle, #HexadecaneWetting, #FlexibleDisplayFilms, #SurfaceEngineering
This is a highlight of the presentation:
Platform Optoelectronic Materials: Flexible, Rollable, Large-Area, Biotech & Beyond
More Highlights from the same talk.
06:28 - 07:22
Why do thinner silver nanowires scatter less light, and what performance do you sacrifice?
Why do thinner silver nanowires scatter less light, and what performance do you sacrifice?
Nanowire geometry is critical for optical applications because it governs how much light the wire scatters. The nanowires discussed here have diameters in the 10 to 20 nanometre range, far smaller than the wavelength of visible light. Yet these nanoparticles still have plasmonic responses: they interact very strongly with a certain energy, a certain wavelength of light.
As the nanowires get thinner, the plasmonic peak shows a pronounced blue shift — visible when comparing generation 5, mass produced at the largest scales, with generation 8, the newest nanowire product. That blue shift means the nanowires scatter much less light and are much less hazy. Thinner wire, therefore, buys a real optical benefit.
The benefit comes with a trade-off. What you sacrifice is yield: nanowire purification becomes more challenging as the wires get thinner. Formulations and growth conditions have to be engineered to drive the different types of nanowires you want to grow, balancing the optical gain against the harder purification and the yield penalty.
In this short video, you can learn:
* Nanowire diameters of 10 to 20 nanometres sit far below the wavelength of visible light, yet the particles still show plasmonic responses that shape how they scatter light.
* Going from generation 5 to generation 8 nanowires produces a pronounced blue shift in the plasmonic peak, which means much less scattered light and much less haze.
* The thinner the nanowire, the more challenging purification becomes and the more yield you give up in exchange for the optical improvement.
📋 **Clip Abstract** Nanowire geometry governs how strongly these plasmonic particles interact with light: at 10 to 20 nanometres the wires are far smaller than visible wavelengths, and thinner generations blue-shift the plasmonic peak so they scatter less light and appear far less hazy. Generation 8 nanowires deliver that lower-haze optical result, but yield drops and purification becomes more challenging than with generation 5.
About the speaker:
* Speaker: Ajay Virkar
* Company: C3Nano
* Event: The Future of Electronics RESHAPED 2022
* Location: Eindhoven, Netherlands
Save the date for the next Future of Electronics RESHAPED conference and exhibition
USA | Mountain View | 9-10 June 2027: https://www.techblick.com/electronicsreshapedusa
Europe | Berlin | 20-21 October 2027: https://www.techblick.com/electronicsreshaped
#SilverNanowire, #PlasmonicBlueShift, #LowHazeCoating, #NanowirePurification, #PrintedElectronics, #TransparentConductors
12:07 - 13:34
Can a nanomaterial ink become conductive in one minute at 25°C on low-Tg plastics and polyurethanes?
Can a nanomaterial ink become conductive in one minute at 25°C on low-Tg plastics and polyurethanes?
The low-temperature LT ink can be coated onto any surface, and within one minute at room temperature it yields a conductive surface. This is aimed at low-Tg or very cheap plastics and biomedical materials such as polyurethanes, whose fundamental temperature limitations are below 40 or 50 degrees Celsius. The standard ink is already low-temperature and fast-curing, but the LT route drives processing lower.
Processing results show conductive coatings applied in one minute at 25 degrees C. The ink covers a wide optoelectronic range; at 40 or 50 ohms per square it shows very nice optical properties even under that one-minute, 25-degree-C cure, with high transmissions and low hazes. Pushing resistance lower can compromise optics, while the lab’s lowest value is about one ohm per square.
That roughly one-ohm-per-square floor is described mostly as an ink and process limitation, not a fundamental one. At the higher 40–50 ohm-per-square range, the one-minute 25-degree-C process retains high transmission and low haze. The trade-off is explicit: lower resistance compromises optics, so the useful window depends on balancing conductivity against optoelectronic performance.
In this short video, you can learn:
* LT ink forms a conductive surface after one minute at room temperature when coated onto a surface.
* The process targets low-Tg and cheap plastics plus biomedical polyurethanes limited below 40–50°C.
* At 40–50 ohms per square, one-minute 25°C coatings show high transmission and low haze; lower resistance trades off optics.
📋 **Clip Abstract** A low-temperature nanomaterial ink can be coated onto surfaces and become conductive within one minute at room temperature, extending electronics to low-Tg plastics and polyurethanes with limits below 40–50°C. Processing at 25°C reaches about one ohm per square in the lab, while 40–50 ohms per square gives high transmission and low haze but lower resistance compromises optics.
About the speaker:
* Speaker: Ajay Virkar
* Company: C3Nano
* Event: The Future of Electronics RESHAPED 2022
* Location: Eindhoven, Netherlands
Save the date for the next Future of Electronics RESHAPED conference and exhibition
USA | Mountain View | 9-10 June 2027: https://www.techblick.com/electronicsreshapedusa
Europe | Berlin | 20-21 October 2027: https://www.techblick.com/electronicsreshaped
#LowTemperatureInk, #OneMinuteCure, #OhmPerSquare, #HighTransmissionLowHaze, #PrintedElectronics, #FlexibleElectronics
09:52 - 11:14
How can metal ion complexes selectively fuse nanowire junctions with silver without melting the one-dimensional structure?
How can metal ion complexes selectively fuse nanowire junctions with silver without melting the one-dimensional structure?
Series resistance in one-dimensional nanomaterial films is dominated by junction resistance between nanowires. The company's approach was to chemically fuse nanowires rather than rely on heat, because truly melting a nanowire destroys its one-dimensional structure and can leave an insulating film. Instead, specific chemistries—metal ions and complexes—are designed to selectively deposit at nanowire junctions.
The junctions are described as local minima in chemical potential, so material wants to go there; thermodynamic and kinetic factors coax the system. At low concentrations, metallic ion complexes are present without an active reduction process. As the ink is coated and solvent dries, the elements concentrate, pushing the reaction to the right; reducing agents convert the complex into metallic silver.
The silver selectively goes to the junctions and fuses them together. This deposits a minimum amount of material right at the junctions, improving their conductivity. The mechanism is presented as a way to address junction resistance in one-dimensional nanomaterials, with the chemistry concentrating and reducing within the drying ink rather than melting the nanowires themselves.
In this short video, you can learn:
* Junction resistance between nanowires dominates the series resistance of one-dimensional nanomaterial films.
* Heat cannot be used to melt nanowires because melting destroys the one-dimensional structure and can produce an insulating film.
* Metal ion and complex chemistries selectively deposit metallic silver at nanowire junctions as the ink dries and concentrates, reducing junction resistance with minimal material.
📋 **Clip Abstract** The clip explains why nanowire films are limited by junction resistance and why melting nanowires with heat is not viable. It describes metal ion and complex chemistries that concentrate as the ink dries, reduce to metallic silver, and selectively deposit at nanowire junctions to fuse them and improve conductivity.
About the speaker:
* Speaker: Ajay Virkar
* Company: C3Nano
* Event: The Future of Electronics RESHAPED 2022
* Location: Eindhoven, Netherlands
Save the date for the next Future of Electronics RESHAPED conference and exhibition
USA | Mountain View | 9-10 June 2027: https://www.techblick.com/electronicsreshapedusa
Europe | Berlin | 20-21 October 2027: https://www.techblick.com/electronicsreshaped
#NanowireJunctionFusing, #MetalIonComplexes, #SelectiveSilverDeposition, #ConductiveInkDrying, #PrintedElectronics, #NanomaterialInks
About this talk
→ Platform Optoelectronic Materials: Flexible, Rollable, Large-Area, Biotech & Beyond · Ajay Virkar · Displays & Lighting: Innovations & Market Trends 2021
Other talks by Ajay Virkar
- A Platform Technology to Revolutionize Electronics and Smart Surfaces: Nanomaterials, Inks, Coatings and Composites · The Future of Electronics RESHAPED 2022
- Platform Optoelectronic Materials: Flexible, Rollable, Large-Area, Biotech & Beyond · Printed, Hybrid, Structural, & 3D Electronics 2021
More highlights from Ajay Virkar
- ▶ Why do thinner silver nanowires scatter less light, and what performance do you sacrifice? · The Future of Electronics RESHAPED 2022
- ▶ How can metal ion complexes selectively fuse nanowire junctions with silver without melting the one-dimensional structure? · The Future of Electronics RESHAPED 2022
- ▶ Can a nanomaterial ink become conductive in one minute at 25°C on low-Tg plastics and polyurethanes? · The Future of Electronics RESHAPED 2022
- ▶ What nanowire loading delivers conductivity competitive with carbon black and CNT fillers? · The Future of Electronics RESHAPED 2022